Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Hot Wire Ignition, HWI = 15 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Cycolac® MG38 ABS
Very high impact ABS. Toughness/rigidity. Good fatigue resistance.
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Cycolac® MG38N ABS (Asia Pacific)
Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)>
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS
Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications.
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Asia Pacific)
Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact for various applications.
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
PLC code 3; UL 746A
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific)
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Lexan® LUX2114G PC (Europe-Africa-Middle East)
Lexan LUX2114G (EXRL0943) is a diffusive, mid viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develope..
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific)
Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop..
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Lexan® LUX2614G PC (Europe-Africa-Middle East)
Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop..
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Lexan® LUX9610 PC (Europe-Africa-Middle East)
Lexan LUX9610 is a UV stabilized flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance providing good colorstab..
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Lexan® LUX9616 PC (Asia Pacific)
Lexan LUX9616 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme..
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Asia Pacific)
Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3..
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer (Asia Pacific)
ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system.
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Asia Pacific)
XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East)
XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS
LNP* Lubricomp* Cycoloy_C2801 compound is a 5% PTFE reinforced PC+ABS, wear resistant, flame retardant compound for moving components in business equipment. Medium heat performance
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS (Asia Pacific)
High impact and ductility at 73F (23C) and -20F (-29C).
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL Rating PLC 3 (15-30 sec)
LG Chemical 20HRI GPPS
Heat resistance, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, S..
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL Rating PLC 3 (15-30 sec)
LG Chemical 65IH HIPS
High impact, Extrusion, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food tray..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=0.750 mm
15 - 30 sec

@Thickness >=0.0295 in
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose
Feature: Injection Molding, PA6+MF23%, High ImpactPA6+GF20%, General PurposeApplication: HMID, SLMP B, HolderCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=0.750 mm
15 - 30 sec

@Thickness >=0.0295 in
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose
Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
PLC code 3; UL 746A
SABIC Innovative Plastics Valox® 325M PBT (Asia Pacific)
325M is a high flow VALOX 325 for restrictive gate tooling (key buttons)This data was supplied by SABIC-IP for the Asia Pacific region.
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East)
VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures.
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Valox® 451E PBT (Asia Pacific)
20% GR. Easy flow version of VALOX 451.
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 3.00 mm
15 - 30 sec

@Thickness 0.118 in
UL Rating PLC 3 (15-30 sec)
Covestro Bayblend® T 45 MN Polycarbonate/ABS Blend
High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy, good platable.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep..
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific)
ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL.
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801R PC+ABS
LNP* Lubricomp* Cycoloy_C2801R compound is a 5% PTFE reinforced PC+ABS wear resistant, flame retardant compound for moving components in business equipment. 30% recycle content.
Copyright © lookpolymers.com All Rights Reserved