Electrical Properties | Metric | English | Comments |
---|---|---|---|
Static Decay | <= 0.010 sec | <= 0.010 sec | 5000V to <50V; FTMS101B |
LNP VALOX® SMV5846 PBT + PET Alloy, 20% Carbon Fiber Reinforcement
(discontinued **) ESD ApplicationsFeatures: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is .. |
|||
Static Decay | <= 0.010 sec | <= 0.010 sec | 5000V to <50V; FTMS101B |
LNP VALOX® SMV5847 PBT + PET Alloy, 30% Carbon Fiber Reinforcement
(discontinued **) ESD Applications. VC3000.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data .. |
|||
Static Decay | <= 0.010 sec | <= 0.010 sec | 5000V to <50V; FTMS101B |
LNP ULTEM® UC3000 Polyetherimide, 30% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |
|||
Static Decay | 0.010 sec | 0.010 sec | 5000V to <50V; FTMS101B |
SABIC Innovative Plastics LNP STAT-KON Cycoloy_JK800 PC+ABS LNP* Stat-kon* Cycoloy_JK800 compound is an 8% carbon fiber reinforcedPC+ABS, electrostatic dissipative ECO conforming FR. Good hydrolytic stability. |
|||
Static Decay | 0.010 sec | 0.010 sec | 5000V to <50V; FTMS101B |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC LNP* Stat-kon* Lexan_LC1500N compound is a 15% carbon fiber, 6% PTFE reinforced polycarbonate. |
|||
Static Decay | 0.010 sec | 0.010 sec | 5000V to <50V; FTMS101B |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Europe-Africa-Middle East) LNP* Stat-kon* Lexan_LCF1506 is a 15% carbon fiber, 6% PTFE reinforced polycarbonate. |
|||
Static Decay | 0.010 sec | 0.010 sec | 5000V to <50V; FTMS101B |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC1010 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* HMC1010 compound is a 10% Carbon fiber reinforced. Static dissipative. Nonbrominated, nonchlornated flame retardant system. UL94 V-1 rated. |
|||
Static Decay | 0.010 sec | 0.010 sec | 5000V to <50V; FTMS101B |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC1010 PPE+PS LNP* Stat-kon* Noryl_HMC1010 compound is a 10% Carbon fiber reinforced. Static dissipative. Nonbrominated, nonchlor- nated flame retardant system. UL94 V-1 rated. |
|||
Static Decay | 0.010 sec | 0.010 sec | 5000V to <50V; FTMS101B |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend. |
|||
Static Decay | 0.010 sec | 0.010 sec | 5000V to <50V; FTMS101B |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+PS LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend. |
|||
Static Decay | 0.010 sec | 0.010 sec | 5000V to <50V; FTMS101B |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC3508 PPE+HIPS (Europe-Africa-Middle East) PRELIMINARY DATA. LNP* Stat-kon* Noryl_NC3508 compound is a 33% glass/mineral/carbon filled PPE+PS. ESD, high heat, tight tolerance: electronic packaging/chip trays. |
|||
Static Decay | 0.010 sec | 0.010 sec | 5000V to <50V; FTMS101B |
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI LNP* Stat-kon* Ultem_UC1200 is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications. |
|||
Static Decay | <= 0.010 sec | <= 0.010 sec | FTMS-101C; 12% R.H., (+5000 V to 50 V) |
Lubrizol Hipscon™ B-515 Static Control Polystyrene Hipscon™ B-515 is a carbon black-filled, Polystyrene compound available in compound form. Hipscom™ B-515 compound maintains extremely low gloss surfaces after molding, allowing for easy reading o.. |
|||
Static Decay | <= 0.010 sec | <= 0.010 sec | FTMS-101C; 12% R.H., (-5000 V to -50 V) |
Lubrizol Hipscon™ B-515 Static Control Polystyrene Hipscon™ B-515 is a carbon black-filled, Polystyrene compound available in compound form. Hipscom™ B-515 compound maintains extremely low gloss surfaces after molding, allowing for easy reading o.. |
|||
Static Decay | <= 0.010 sec | <= 0.010 sec | FTMS-101C; 12% R.H., (+5000 V to 50 V) |
Lubrizol Hipscon™ M-505 Static Control High Impact Polystyrene Hipscon™ M-505 is a conductive, carbon black filled, High Impact Polystyrene available as extruded sheet. Thermoformed trays are lightweight and easily formed into deep pockets that maintain unifo.. |
|||
Static Decay | <= 0.010 sec | <= 0.010 sec | FTMS-101C; 12% R.H., (-5000 V to -50 V) |
Lubrizol Hipscon™ M-505 Static Control High Impact Polystyrene Hipscon™ M-505 is a conductive, carbon black filled, High Impact Polystyrene available as extruded sheet. Thermoformed trays are lightweight and easily formed into deep pockets that maintain unifo.. |
|||
Static Decay | <= 0.010 sec | <= 0.010 sec | FTMS-101C; 12% R.H., (-5000 V to -50 V) |
Lubrizol Hipscon™ M-530 Static Control Polystyrene Hipscon™ M-530 is a conductive, carbon black filled, polystyrene available as extruded sheet and compound. Thermoformed trays are lightweight and easily formed into deep pockets that maintain unif.. |
|||
Static Decay | 0.010 sec | 0.010 sec | 12% RH (-5000 V to -50 V); FTMS-101C |
Lubrizol STAT-RITE® S-1100 Static Dissipative TPU Description: Stat-Rite® S1100 is a static dissipative TPU alloy. Stat-Rite S-1100 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD p.. |
|||
Static Decay | 0.010 sec | 0.010 sec | FTMS-101C; 12% R.H., (+5000 V to 50 V) |
Lubrizol Stat-Rite® S-250 Static Control Polypropylene Stat-Rite® S-250 is a static dissipative Polypropylene alloy. Stat-Rite S-250 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD pr.. |
|||
Static Decay | 0.010 sec | 0.010 sec | FTMS-101C; 12% R.H., (-5000 V to -50 V) |
Lubrizol Stat-Rite® S-250 Static Control Polypropylene Stat-Rite® S-250 is a static dissipative Polypropylene alloy. Stat-Rite S-250 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD pr.. |
|||
Static Decay | 0.010 sec | 0.010 sec | FTMS-101C; 12% R.H., (+5000 V to 50 V) |
Lubrizol Stat-Rite® S-680 Static Control PETG Alloy Stat-Rite® S-680 is a static dissipative PETG alloy. Stat-Rite® M-680 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio.. |
|||
Static Decay | 0.010 sec | 0.010 sec | FTMS-101C; 12% R.H., (-5000 V to -50 V) |
Lubrizol Stat-Rite® S-680 Static Control PETG Alloy Stat-Rite® S-680 is a static dissipative PETG alloy. Stat-Rite® M-680 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio.. |
|||
Static Decay | 0.010 sec | 0.010 sec | FTMS-101C; 12% R.H., (-5000 V to -50 V) |
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ES.. |
|||
Static Decay | <= 0.010 sec | <= 0.010 sec | 5000V to <50V; FTMS101B |
LNP ULTEM® SMU5831 Polyetherimide, 30% CarbonGlassMineral Reinforced
(discontinued **) ESD characteristics for ultra high-heat applications. Will be UC3010H.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compa.. |
|||
Static Decay | <= 0.010 sec | <= 0.010 sec | 5000V to <50V; FTMS101B |
LNP ULTEM® SMU5852 Polyetherimide, 30% Carbon Fiber Reinforcement, 15% PTFE Lubricant
(discontinued **) Features: Lubricated, Electrically Conductive, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Dis.. |
|||
Static Decay | 0.010 sec | 0.010 sec | FTMS-101C; 12% R.H. (+5000 V to 50 V) |
Lubrizol Stat-Rite® SIS535 Static Control System Product Description: Stat-Rite® SIS535 is a static dissipative HIPS alloy. Stat-Rite SIS535 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, perma.. |
|||
Static Decay | 0.010 sec | 0.010 sec | (-5000 V to -50 V) |
Lubrizol Stat-Rite® SIS535 Static Control System Product Description: Stat-Rite® SIS535 is a static dissipative HIPS alloy. Stat-Rite SIS535 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, perma.. |
|||
Static Decay | <= 0.010 sec | <= 0.010 sec | 5000V to <50V; FTMS101B |
LNP ULTEM® SMU5834 Polyetherimide, 20% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |
|||
Static Decay | <= 0.010 sec | <= 0.010 sec | 5000V to <50V; FTMS101B |
LNP ULTEM® SMU5836 Polyetherimide, 30% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |
|||
Static Decay | 0.010 sec | 0.010 sec | 5000V to <50V; FTMS101B |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |