Polymer Property : Static Decay = 2.00 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:5
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:5
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:13
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini..
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:4
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:3
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:3
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:4
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:6
Overview of materials for Nylon 6, Stainless Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o..
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:7
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim..
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:3
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:5
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:13
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi..
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:4
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:3
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..