Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® LDPE - Low Density Polyethylene (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® PP Natural Co-Polymer Polypropylene (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® PP, Black Homopolymer Polypropylene (ASTM Product Data Sheet) High impact resistance strength Better resistance to cracking at low temperatures than Homopolymer Polypropylene More pliable than homopolymer Meets food handling guidelines Chemical- and corrosion.. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® PP, Natural Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW-PE, Natural & Colored Except Black (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP TIVAR® 88-2 UHMW-PE, Premium Lubricant Filled Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic f.. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP TIVAR® Dockguard - UHMW-PE - Black UV Stabilized UHMW-PE (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | ASTM D257 |
PolyOne Edgetek® PS-20GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Sanalite® HDPE - High Density Polyethylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | VDE 0303 |
GEHR Plastics PEEK Polyetheretherketone Polyether etherketone can be used at very high temperatures and it shows good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical re.. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | VDE 0303 |
GEHR Plastics PEI Polyetherimide Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance, good dimensional stability and creep resistance. Its unique torque strength permits the economic.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | IEC 60093 |
Westlake Plastics MediPEEK IM Polyetheretherketone for Medical Applications MediPEEK-IM is a high performance semi-crystalline thermoplastic designed for long term body contact as an implantable material. It is USP Class VI and compliant to ASTM F2026. It has excellent st.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | IEC 60093 |
Westlake Plastics MediPEEK T Polyetheretherketone for Medical Applications MediPEEK-T is a high performance semi-crystalline thermoplastic designed for short term body contact as an implantable material. It is USP Class VI and ASTM F2026 compliant. It has excellent steri.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Dry; ASTM D257 |
DuPont™ Nomex® 419 Paper, 7 mil Nominal Thickness Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 23.0 °C |
1.00e+15 ohm @Temperature 73.4 °F |
IEC 60093 |
Ensinger TECASINT™ 2021 Polyimide, Brown (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® 475 Polyester Film, 200 Gauge Melinex® 475 is a high yield, translucent polyester film with superb handling properties. Both surfaces are pretreated to promote adhesion to most industrial coatings.General Product Info: This fil.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® S Polyester Film, 200 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® S Polyester Film, 400 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® S Polyester Film, 500 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 200 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 300 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 400 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 48 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 500 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 92 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Adhesive side; ASTM D257 |
3M 4104 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® White Homopolymer Polypropylene (ASTM Product Data Sheet) |