Material Notes:
Melinex® 475 is a high yield, translucent polyester film with superb handling properties. Both surfaces are pretreated to promote adhesion to most industrial coatings.General Product Info: This film has low extractables and a high tear strengthApprovals: UL Recognition - Product has been registered with Underwriters LaboratoriesInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 82.7 MPa
12000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 82.7 MPa
12000 psi
ASTM D882A
Film Elongation at Break, MD 180 %
180 %
ASTM D882A
Film Elongation at Break, TD 110 %
110 %
ASTM D882A
Coefficient of Friction, Dynamic 0.30
0.30
Film Tensile Strength at Break, MD 159 MPa
23000 psi
ASTM D882A
Film Tensile Strength at Break, TD 179 MPa
26000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 3.0 %

@Temperature 190 °C,
Time 300 sec
3.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 0.50 %

@Temperature 190 °C,
Time 300 sec
0.50 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Gloss 60 %
60 %
45°, A side; ASTM D1003
95 %
95 %
45°, B side; ASTM D1003
Transmission, Visible 40 %
40 %
TLT; ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm

@Temperature 25.0 °C
1.00e+17 ohm-cm

@Temperature 77.0 °F
100 V DC 50% RH, 1000 sec electrification time; ASTM D257
Surface Resistivity per Square 1.00e+15 ohm

@Temperature 25.0 °C
1.00e+15 ohm

@Temperature 77.0 °F
500 V DC @ 50% RH; ASTM D257
Users viewing this material also viewed the following: