Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® S Polyester Film, 500 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for the full range of Melinex® applications. Approvals: UL 94 VTM-2 - for 92 - 500 gauge (0.023 - 0.13mm) and UL Recognition - Product has been registered with Underwriters LaboratoriesInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 100 MPa
14500 psi
ASTM D882A
Film Tensile Strength at Yield, TD 99.3 MPa
14400 psi
ASTM D882A
Film Elongation at Break, MD 160 %
160 %
ASTM D882A
Film Elongation at Break, TD 100 %
100 %
ASTM D882A
Coefficient of Friction, Dynamic 0.40
0.40
A-B; ASTM D1894
Film Tensile Strength at Break, MD 200 MPa
29000 psi
ASTM D882A
Film Tensile Strength at Break, TD 255 MPa
37000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 0.50 %

@Temperature 190 °C,
Time 300 sec
0.50 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze 20.7 %
20.7 %
ASTM D1003
Transmission, Visible 81 %
81 %
TLT; ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm

@Temperature 25.0 °C,
Time 100 sec
1.00e+17 ohm-cm

@Temperature 77.0 °F,
Time 0.0278 hour
100 V DC; ASTM D257
Surface Resistivity per Square 1.00e+15 ohm

@Temperature 25.0 °C
1.00e+15 ohm

@Temperature 77.0 °F
500 V DC @ 50% RH; ASTM D257
Dielectric Strength 126 kV/mm
3200 kV/in
0.25 inch electrodes in dry air @25°C; ASTM D149-81
Dielectric Breakdown 16000 V
16000 V
0.25 inch electrodes in dry air @25°C; ASTM D149-81