Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 180 V | 180 V | UL 746 |
Solvay Specialty Polymers Mindel® B-430 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-430 is a 30% glass reinforced thermoplastic with excellent dimensional stability, exceptional resistance to warp, good chemical resistance, and high stiffness. It was developed specifically.. |
|||
Comparative Tracking Index | 180 - 225 V | 180 - 225 V | Average value: 191 V Grade Count:10 |
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum .. |
|||
Comparative Tracking Index | 180 V | 180 V | UL 746 |
Plenco 504 Black (INJ) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)< Plaslok 504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding compounds. Since it also has good electrical.. |
|||
Comparative Tracking Index | 180 V | 180 V | UL 746 |
Plenco 306 Black General Purpose Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 306 is a two-stage, mineral and flock-filled phenolic molding compound designed to have the heat resistant characteristics of Plaslok 504, while at the same time, improved impact strength.Da.. |
|||
Comparative Tracking Index | 180 V | 180 V | UL 746 |
Plenco 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 308 is a two-stage, mineral and flock-filled phenolic molding compound designed to withstand the hostile environment of high abrasion and high tangential speed of engine pulleys. It is char.. |
|||
Comparative Tracking Index | 180 V | 180 V | UL 746 |
Plenco 308 Black (INJ) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 308 is a two-stage, mineral and flock-filled phenolic molding compound designed to withstand the hostile environment of high abrasion and high tangential speed of engine pulleys. It is char.. |
|||
Comparative Tracking Index | 180 V | 180 V | UL 746 |
Plenco 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok 309 is a two-stage, mineral and fiber-filled phenolic molding compound having excellent impact strength; and as such, is considered a good candidate for replacing chopped-fiber filled compou.. |
|||
Comparative Tracking Index | 180 V | 180 V | UL 746 |
Plenco 309 Black (INJ) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok 309 is a two-stage, mineral and fiber-filled phenolic molding compound having excellent impact strength; and as such, is considered a good candidate for replacing chopped-fiber filled compou.. |
|||
Comparative Tracking Index | 180 V | 180 V | UL 746 |
Plaslok 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 308 is a two-stage, mineral and flock.. |
|||
Comparative Tracking Index | 180 V | 180 V | UL 746 |
Plaslok 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber.. |
|||
Comparative Tracking Index | 180 V | 180 V | UL 746 |
Plaslok 309 Black (INJ) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber.. |
|||
Comparative Tracking Index | 180 V @Thickness 3.17 mm |
180 V @Thickness 0.125 in |
ASTM D3638 |
Industrial Laminates/Norplex NP611 Paper Base Laminate Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a.. |
|||
Comparative Tracking Index | 180 V @Thickness 3.17 mm |
180 V @Thickness 0.125 in |
ASTM D3638 |
Industrial Laminates/Norplex NP680 Paper Base Laminate Description: Hot punching grade with electrical properties between NP611 to NP631.Thickness Tested: 0.062", 0.125" & 0.500" |
|||
Comparative Tracking Index | 180 V @Thickness 3.17 mm |
180 V @Thickness 0.125 in |
ASTM D3638 |
Industrial Laminates/Norplex NP625 Paper Base Laminate Description: Paper phenolic grade with better moisture resistance than NP612. Requires less heat to punch and shear than NP611. |
|||
Comparative Tracking Index | 180 V @Thickness 3.17 mm |
180 V @Thickness 0.125 in |
ASTM D3638 |
Industrial Laminates/Norplex NP664 Paper Base Laminate Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062.. |
|||
Comparative Tracking Index | 180 V | 180 V | IEC Tracking Index |
Sumitomo Bakelite Durez® 156 Phenolic, Compression Grade Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL.. |
|||
Comparative Tracking Index | 180 V | 180 V | IEC Tracking Index |
Sumitomo Bakelite Durez® 156 Phenolic, Injection Grade Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL.. |
|||
Comparative Tracking Index | 180 V | 180 V | VDE 0303-P1, IEC 112 |
EPICHEM Epilon FR-PC V0 Polycarbonate Characteristics: self-extinguishing V0 at 1,6 mm |
|||
Comparative Tracking Index | 180 V | 180 V | VDE 0303-P1, IEC 112 |
EPICHEM Epilon PC IX3000 Polycarbonate, High Impact Characteristics: high fluidity, high impact |
|||
Comparative Tracking Index | >= 180 V | >= 180 V | IEC 1212-2 6.4 |
Hippe EP GC 203 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Comparative Tracking Index | >= 180 V | >= 180 V | IEC 1212-2 6.4 |
Hippe EP GC 204 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Comparative Tracking Index | >= 180 V | >= 180 V | IEC 1212-2 6.4 |
Hippe EP GC 205 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Comparative Tracking Index | 180 V | 180 V | VDE 0303-P1, IEC 112 |
EPICHEM Epicarb PC Polycarbonate Characteristics: high fluidity, good impact |
|||
Comparative Tracking Index | >= 180 V | >= 180 V | IEC 1212-2 6.4 |
Hippe EP GM 203 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Comparative Tracking Index | >= 180 V | >= 180 V | IEC 1212-2 6.4 |
Hippe EP GM 204 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Comparative Tracking Index | 180 - 600 V | 180 - 600 V | Average value: 280 V Grade Count:28 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Comparative Tracking Index | 180 V | 180 V | UL 746 |
Plaslok 504 Black (COM) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)&l Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 504 is a two-stage, mineral and cellu.. |
|||
Comparative Tracking Index | 180 V | 180 V | UL 746 |
Plaslok 504 Black (INJ) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)&l Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 504 is a two-stage, mineral and cellu.. |
|||
Comparative Tracking Index | 180 V | 180 V | UL 746 |
Plaslok 306 Black General Purpose Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 306 is a two-stage, mineral and flock.. |
|||
Comparative Tracking Index | 180 V | 180 V | UL 746 |
Plaslok 308 Black (INJ) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 308 is a two-stage, mineral and flock.. |