Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
Qualchem Danamid FES-23 HUV Polyamide 6 Impact resistant, cold. Heat and UV stabilized, for long-lasting use at 120-130°C, protected against artificial light.Information provided by Qualchem Zrt. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Comparative Tracking Index | 525 - 600 V | 525 - 600 V | Average value: 588 V Grade Count:13 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
DSM Akulon® S224-KMV7 Nylon 66-35% Mineral Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
DSM Akulon® S224-KMV7 Nylon 66-35% Mineral Reinforced (European and Asian Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 525 - 600 V | 525 - 600 V | Average value: 586 V Grade Count:61 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Comparative Tracking Index | 525 V | 525 V | d.a.m.; Solution A; IEC 60112 |
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Comparative Tracking Index | 525 V | 525 V | d.a.m.; Solution A; IEC 60112 |
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
Lanxess Durethan® BKV 30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade with 30% glass fibers, good heat-ageing resistance |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
Lanxess Durethan® BM 240 H2.0 901510 Nylon 6, 40% Mineral PA 6, injection molding grade, 40% mineral, isotopic properties, good heat-ageing resistance |
|||
Comparative Tracking Index | 525 V | 525 V | A solution |
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Comparative Tracking Index | 525 V | 525 V | Solution A; IEC 60112 |
Solvay TECHNYL® B 218 Black 21 N PA66/6, DRY Description: Unreinforced copolyamide PA 66/6 , heat stabilized , medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® B 218 offers all of the primary proper.. |
|||
Comparative Tracking Index | 525 V | 525 V | Solution B; IEC 60112 |
Solvay TECHNYL® A 216 V15 Black 21N PA66, 15% glass fiber, DRY Description: Polyamide PA66, reinforced with 15% of glass fiber, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 216 V15 is used in all sectors of industry, offer.. |
|||
Comparative Tracking Index | 525 V | 525 V | Solution B; IEC 60112 |
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, DRY Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and.. |
|||
Comparative Tracking Index | 525 V | 525 V | ASTM D3638 |
Plenco 00755 Melamine-Phenolic, Granular, Injection Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Comparative Tracking Index | 525 V | 525 V | GB4207 |
Zhejiang Juner PA-A6 GF20% Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Comparative Tracking Index | 525 V | 525 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® BGM-40 X PA6-(GF+MD)40 Product description: Grilon BGM-40 X is a heat stabilized PA 6 injection molding grade with a 40 % reinforcement combination (mineral and glass fiber). Grilon BGM-40 X has the following important pr.. |
|||
Comparative Tracking Index | 525 V | 525 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® TSG-50/4 W PA666-GF50 Product description: Grilon TSG-50/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Comparative Tracking Index | 525 V @Thickness 3.00 mm |
525 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Comparative Tracking Index | 525 V @Thickness 3.00 mm |
525 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Comparative Tracking Index | 525 V | 525 V | Test solution A; IEC 60112 |
BASF Ultramid® FRee B3U31G4 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Comparative Tracking Index | 525 V @Thickness 3.00 mm |
525 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Comparative Tracking Index | 525 V | 525 V | Test solution A; IEC 112 |
BASF Ultradur® FRee B 4440 G5 25% Glass Filled PBT Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so.. |
|||
Comparative Tracking Index | 525 V @Thickness 3.00 mm |
525 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
Azoty Tarnow™ Tarnamid® T-27 GF25 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 25% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
Lanxess Pocan® DP B 3235 XF 901510 PBT, 30% Glass Fiber
(discontinued **) PBT, 30% glass fibers, injection molding, improved flowability |