Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | At 8-20% Dosing; ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® ESD 5000 Polyolefin Compatible Dissipative Masterbatch, IDP Additive PRE-ELEC® ESD 5000 is a polyolefin compatible dissipative masterbatch developed for PP injection moulded products. The active substance is an IDP (inherently dissipative polymer) and it gives a per.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | Average value: 1.00e+8 ohm Grade Count:5 |
Overview of materials for Phenolic, Novolac, Fabric Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values .. |
|||
Surface Resistance | 1.00e+8 - 8.00e+15 ohm | 1.00e+8 - 8.00e+15 ohm | Average value: 8.06e+14 ohm Grade Count:38 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Surface Resistance | 1.00e+8 - 1.00e+16 ohm | 1.00e+8 - 1.00e+16 ohm | Average value: 7.50e+15 ohm Grade Count:4 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Surface Resistance | <= 1.00e+8 ohm | <= 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 1105-7678 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Surface Resistance | <= 1.00e+8 ohm | <= 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 1105-8160 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Surface Resistance | <= 1.00e+8 ohm | <= 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 1105-8167 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Surface Resistance | >= 1.00e+8 ohm | >= 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 1-8181 Polyamide 66, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec.. |
|||
Surface Resistance | >= 1.00e+8 ohm | >= 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 1-8218 Polyamide 66, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec.. |
|||
Surface Resistance | >= 1.00e+8 ohm | >= 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 1850-7431 PBT, with carbon fiber and glass spheres Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low warpage.Low waterabsorbtion, for dimensional stable precision parts.Par.. |
|||
Surface Resistance | >= 1.00e+8 ohm | >= 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 1-8520 Polyamide 66, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | Injection molded parts |
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNT.. |
|||
Surface Resistance | >= 1.00e+8 ohm | >= 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 20-8254 Polyphthalamide, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Surface Resistance | <= 1.00e+8 ohm | <= 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 3-7723/ EG Polyamide 6, with carbon fiber, high viscosity Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressAntistatic.Handles, levers, rolle.. |
|||
Surface Resistance | <= 1.00e+8 ohm | <= 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 50/CF/7/GF/20/TF/10/BK Polycarbonate, with carbon fiber, glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | ASTM D257 |
LG Chemical LUCON CP-4201F Conductive Thermoplastic, Flame Retardant LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | IEC 60093 |
Menzolit Menzolit® BMC 2600 Unsaturated Polyester UP BMC 2600 is a special BMC with reduced electrical properties. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. Because of its improved.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | |
LATI Latiohm 62-09 PD01 G/20-V2HF PA6, 20% Glass Fiber Reinforced, Flame Retardant Semiconductive/dissipative product based on Polyamide 6 (PA6). Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties.Availabili.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | |
LATI Latiohm 66-08 PD02 G/35 PA66, 35% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | |
LATI Latiohm 75/4-10 CNT PBT Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | DIN 53482 |
Schwartz Technical Plastics LAMINEX® 2000 Cotton Fabric, Phenolic Resin Impregnated, Coarse Application: rollneck-bearings, coverts for friction rollsInformation provided by Schwartz Technical Plastics GmbH |
|||
Surface Resistance | 1.00e+8 - 1.00e+10 ohm | 1.00e+8 - 1.00e+10 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS (Asia Pacific) LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D257 |
Techmer ES Statiblend® 02056 BKN Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9109116Information provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+8 - 1.00e+11 ohm | 1.00e+8 - 1.00e+11 ohm | ASTM D257 |
Techmer ES Statiblend® HIPS E Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveAppearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+8 - 1.00e+11 ohm | 1.00e+8 - 1.00e+11 ohm | ASTM D257 |
Techmer ES Statiblend® PA6/6 GF10 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: LubricantFeatures: Conductive and LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® LC108 PC (Asia Pacific) Polycarbonate base, 8% carbon fiber reinforced, FR |