Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | >= 1.00e+9 ohm | >= 1.00e+9 ohm | IEC 60093 |
Murtfeldt Muralen® Black Antistatic Polyethylene, Conductive Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+10 ohm | 1.00e+9 - 1.00e+10 ohm | At 20-25% Dosing; ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® ESD 6010 Dissipative Masterbatch, IDP Additive PRE-ELEC® ESD 6010 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro.. |
|||
Surface Resistance | <= 1.00e+9 ohm | <= 1.00e+9 ohm | ASTM D257 |
PolyOne Bergamid™ XP6042701 Polyamide 6 (Nylon 6) Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3.5 sec Cycle Time: 18 to 60 secInformation provided by PolyOne |
|||
Surface Resistance | 1.00e+9 - 1.00e+13 ohm | 1.00e+9 - 1.00e+13 ohm | ASTM D257 |
PolyOne Stat-Tech™ AS-15GF/000 SD ABS - 15% Glass Fiber Reinforced - Antistatic Protection
(discontinued **)& Data provided by PolyOne. |
|||
Surface Resistance | 1.00e+9 - 1.00e+16 ohm | 1.00e+9 - 1.00e+16 ohm | Average value: 2.84e+15 ohm Grade Count:19 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Surface Resistance | >= 1.00e+9 ohm | >= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 1105-8382 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Highly dimensionally stable at ele.. |
|||
Surface Resistance | <= 1.00e+9 ohm | <= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 20-7913 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Surface Resistance | <= 1.00e+9 ohm | <= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 20-8286 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Surface Resistance | >= 1.00e+9 ohm | >= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 6-7833 Polyamide 12, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion, for dimensional stable precision parts.Isotropic sh.. |
|||
Surface Resistance | >= 1.00e+9 ohm | >= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 6-8548 Polyamide 12, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Suitable for discharging of statically generated electricity.Dynamic stressed parts.Low waterab.. |
|||
Surface Resistance | 1e+05 - 1.00e+9 ohm | 1e+05 - 1.00e+9 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX05499 PC (Asia Pacific) LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 1.00e+9 - 1.00e+14 ohm | 1.00e+9 - 1.00e+14 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KE004 is a compound based on Acetal Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS LNP STAT-LOY* A3000 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS LNP* STAT-LOY* A30009 is a compound based on ABS. Added features of this material include: Antistatic, Flame Retardant. |
|||
Surface Resistance | 1.00e+9 ohm | 1.00e+9 ohm | ASTM D257 |
Techmer ES Statiblend® ABS E AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Surface Resistance | 1.00e+9 - 3.16e+9 ohm | 1.00e+9 - 3.16e+9 ohm | IS 3396-1979 |
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium.. |
|||
Surface Resistance | 1.00e+9 ohm | 1.00e+9 ohm | IEC 60093 |
Hexion Bakelite™ PF 4010 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage
(disconti Glass fiber reinforced and inorganically filled molding compound. High heat resistance, reduced molding shrinkage, good chemical resistance and mechanical properties.Application areas: Switch housi.. |