Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000100 ohm-cm @Temperature 300 °C |
0.000100 ohm-cm @Temperature 572 °F |
|
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Electrical Resistivity | 0.000100 ohm-cm | 0.000100 ohm-cm | RT |
Outokumpu 353MA® High Temperature Austenitic Stainless Steel Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but.. |
|||
Electrical Resistivity | 0.000100 ohm-cm | 0.000100 ohm-cm | RT |
Outokumpu 4529 Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Electrical Resistivity | 0.000100 ohm-cm @Temperature 300 °C |
0.000100 ohm-cm @Temperature 572 °F |
|
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Electrical Resistivity | 0.000100 ohm-cm @Temperature 300 °C |
0.000100 ohm-cm @Temperature 572 °F |
|
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Electrical Resistivity | 0.000100 - 1.00e+14 ohm-cm | 0.000100 - 1.00e+14 ohm-cm | Average value: 7.14e+13 ohm-cm Grade Count:7 |
Overview of materials for Silicone Foam This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Electrical Resistivity | 0.000100 ohm-cm @Temperature 20.0 °C |
0.000100 ohm-cm @Temperature 68.0 °F |
|
Industeel SIRIUS 800 H+ Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at t.. |
|||
Electrical Resistivity | 0.000100 ohm-cm @Temperature 20.0 °C |
0.000100 ohm-cm @Temperature 68.0 °F |
|
Industeel URANUS® B28 High Nickel Super-Austenitic Stainless Steel Description: URANUS® B28 (UR B28) is a super-austenitic stainless steel with very high nickel (31%) and chromium (27%) contents. The molybdenum content is about 3.5%. The alloy is designed for sp.. |
|||
Electrical Resistivity | 0.000100 ohm-cm @Temperature 20.0 °C |
0.000100 ohm-cm @Temperature 68.0 °F |
|
Industeel URANUS® B66 High Strength Super-Austenitic Stainless Steel with PREN = 54 Description: Research carried out these last five years has shown that combined additions of chromium, tungsten, molybdenum, nitrogen and copper, make it possible to design a super-austenitic stainl.. |
|||
Electrical Resistivity | 0.000100 ohm-cm @Temperature 20.0 °C |
0.000100 ohm-cm @Temperature 68.0 °F |
|
Industeel SIRIUS 800 Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at t.. |
|||
Electrical Resistivity | <= 0.000100 ohm-cm | <= 0.000100 ohm-cm | Cured |
Atom Adhesives AA-DUCT 902 Epoxy Adhesive and Coating AA-DUCT 902 is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of.. |
|||
Electrical Resistivity | 0.000100 ohm-cm @Temperature 20.0 °C |
0.000100 ohm-cm @Temperature 68.0 °F |
|
Industeel SIRIUS 800 H Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at tempe.. |
|||
Electrical Resistivity | 0.000100 ohm-cm | 0.000100 ohm-cm | RT |
Outokumpu 904L High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Electrical Resistivity | 0.000100 ohm-cm @Temperature 300 °C |
0.000100 ohm-cm @Temperature 572 °F |
|
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Electrical Resistivity | 0.000100 ohm-cm | 0.000100 ohm-cm | |
Special Metals INCOLOY® 27-7MO Super-Austenitic Stainless Steel INCOLOY® alloy 27-7MO (UNS S31277; EP 1,263,999 B1) is an advanced 7% molybdenum super-austenitic stainless steel offering corrosion resistance in most environments superior to 6% molybdenum super-.. |