Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | Average value: 1.00e+17 ohm-cm Grade Count:8 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report.. |
|||
Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
NOVA Chemicals Sclair® 35BE HDPE Extrusion Resin
(discontinued **) Features: Medium molecular weight HDPE, excellent ESCR, excellent toughness, good processability, outstanding abrasion resistance.Applications: Extrusion on to metal pipes to produce a corrosion res.. |
|||
Electrical Resistivity | 1.00e+17 - 2.60e+17 ohm-cm | 1.00e+17 - 2.60e+17 ohm-cm | Average value: 2.13e+17 ohm-cm Grade Count:6 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Electrical Resistivity | 1.00e+17 - 1.00e+18 ohm-cm | 1.00e+17 - 1.00e+18 ohm-cm | Average value: 8.94e+17 ohm-cm Grade Count:17 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Electrical Resistivity | 1.00e+17 - 1.00e+18 ohm-cm | 1.00e+17 - 1.00e+18 ohm-cm | Average value: 9.55e+17 ohm-cm Grade Count:10 |
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu.. |
|||
Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
Cosmic Plastics K31 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
Cosmic Plastics K61 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
Cosmic Plastics K77 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
DuPont™ Kapton® 100ZT Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available i.. |
|||
Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
DuPont™ Kapton® 300FPC Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick.. |
|||
Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
DuPont™ Kapton® 300KN Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dian.. |
|||
Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
DuPont™ Kapton® 500A Polyimide Film, 125 Micron Thickness Film thickness 125 micron (5.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an .. |
|||
Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
DuPont™ Kapton® 500FPC Polyimide Film, 125 Micron Thickness Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thic.. |
|||
Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
DuPont™ Kapton® 50EN Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications req.. |
|||
Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
DuPont™ Kapton® 50FPC Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick.. |
|||
Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
DuPont™ Kapton® 50KN Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dian.. |
|||
Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
DuPont™ Kapton® 50ZT Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available i.. |
|||
Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | per ASTM D257-91 for Kapton® HN |
DuPont™ Kapton® 200ZT Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available in.. |
|||
Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | IEC 60093 |
CENTROPLAST CENTROPHEN Polyphenylene ether modified This material is a lightweight plastic with low moisture absorption, and is impact resistant at low temperatures. Applications include fittings, drive components for domestic appliances, and compon.. |
|||
Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
Cosmic Plastics 6120F Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | Average value: 1.00e+17 ohm-cm Grade Count:4 |
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma.. |
|||
Electrical Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | IEC 60093 |
CENTROPLAST CENTROSOL Acrylonitrile butadiene Styrene copolymer CENTROSOL ABS has high rigidity and hardness even at low temperatures. It is scratch resistant, non-toxic, with high surface resistance. It is used in operation components for electrical equipment .. |
|||
Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
Cosmic Plastics 224 Dacron Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
Cosmic Plastics 6160 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
Cosmic Plastics 6230F Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
Cosmic Plastics D44 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |