Material Notes:
CENTROSOL ABS has high rigidity and hardness even at low temperatures. It is scratch resistant, non-toxic, with high surface resistance. It is used in operation components for electrical equipment and precision mechanics.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.20 %
0.20 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 1.0 %
1.0 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Hardness, Rockwell M 114

@Thickness 10.0 mm
114

@Thickness 0.394 in
ISO 2039-2
Ball Indentation Hardness 98.0 MPa
14200 psi
value at 30 sec.; ISO 2039-1
Tensile Strength at Break 40.0 MPa
5800 psi
v = 5 mm/min; ISO 527-2
Tensile Strength, Yield 55.0 MPa
7980 psi
v = 50 mm/min; ISO 527-2
Elongation at Break 5.0 %
5.0 %
ISO 527-2
Tensile Modulus 2.60 GPa
377 ksi
ISO 527-2
Flexural Modulus 2.50 GPa
363 ksi
ISO 178
Charpy Impact, Notched 2.50 J/cm²
11.9 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
Melting Point 235 °C
455 °F
10K/min; ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75-2
Vicat Softening Point 101 °C
214 °F
VST/B/50; ISO 306
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
HB

@Thickness 6.00 mm
HB

@Thickness 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Dielectric Constant 2.6

@Frequency 1e+6 Hz
2.6

@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 18.0 kV/mm
457 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.0080

@Frequency 1e+6 Hz
0.0080

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V