Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
UL 746 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.70 mm |
60 - 120 arcs @Thickness 0.0669 in |
UL 746 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
UL 746 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10FR-(VIK) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Impact Modifier and Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-(22) 22 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-(IM) 10 MFI Impact Modified Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-CL(15) 15 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10FR-(V16) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10FR-(V18) 18 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 2.50 mm |
60 - 120 arcs @Thickness 0.0984 in |
PLC 1 |
PTS Tristar® PC-10FRN 15 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-CL02(V38) 38 MFI Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1; UL 746 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**) Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
(ALL) |
Hexion Bakelite™ PF 2400 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof, UL Listed
(disc Phenolic molding compound, inorganically/organically filled, average heat resistance, increased dimensional stability, dish washer proof, UL listed molding compound 1.5 mm/V-0 (ALL).Application area.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
(BK) |
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical HI100K ABS, High Impact Feature: Injection Molding, High Impact, Good ProcessingApplication: Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical LUMAX GP5306F PBT+ABS+GF30%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF30%, Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 and 1309-64-4Information provided by LG .. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical Lupox® GP2306FB PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical Lupoy 1301V-10 Polycarbonate Resin Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
|
LG Chemical Lupoy 1301V-10 Polycarbonate Resin Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical PT270 ABS Feature: Injection Molding, Good PaintabilityApplication: Exterior Part of Automobile and Motor cycleCAS No. 9003-56-9Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 0.710 mm |
60 - 120 arcs @Thickness 0.0280 in |
|
LG Chemical Lupox® GP2306FG PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |