Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Wire & Cable 3701-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Wire & Cable JJX20A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1104L-xx60FRDUV Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJJX206L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 166 - 174 °C | 331 - 345 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJMF113L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
S&E Specialty Polymers TufTech™ GA-92-129 Clear PVC Compound Application: A clear, PVC-based compound designed for speaker wire applications.Information provided by S&E Specialty Polymers |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible A6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible B65B0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible B65B1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
PolyOne Geon™ Vinyl Flexible R5145B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Huntsman PE1041 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good optical, medium impact strength, and good processability.Applications: Film extrusion: general purpose packaging.FDA Notes: Conforms to FDA regulation 2.. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Huntsman PE1065 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA regu.. |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible 86280 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible B6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible B65U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible C6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible C6501 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible H43356A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 160 - 174 °C | 320 - 345 °F | |
PolyOne Geon™ Vinyl Flexible R263AM Polyvinyl Chloride + NBR (PVC+NBR) Information provided by PolyOne |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 8600-75 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 8915-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 8925-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 8940-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 8950-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 8980-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 9077-75 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 9915-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 9940-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 9980-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |