| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Flexible A6500 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.023 - 0.027 cm/cm | 0.023 - 0.027 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 58 | 58 | 15 sec; ASTM D2240 |
| 65 | 65 | ASTM D2240 | |
| Tensile Strength at Break | 9.65 MPa | 1400 psi | 510 mm/min; ASTM D638 |
| Tensile Strength | 3.93 MPa <br>@Strain 100 % |
570 psi <br>@Strain 100 % |
510 mm/min; ASTM D638 |
| Elongation at Break | 440 % | 440 % | 510 mm/min; ASTM D638 |
| Tear Strength | 29.8 kN/m | 170 pli | Die C, 510 mm/min; ASTM D624 |
| Compression Set | 30 % <br>@Temperature 23.0 °C,<br> Time 79200 sec |
30 % <br>@Temperature 73.4 °F,<br> Time 22.0 hour |
ASTM D395 |
| Clash Berg Modulus | 0.0379 GPa | 5.50 ksi | ASTM D1043 |
| 0.310 GPa <br>@Temperature -40.0 °C |
45.0 ksi <br>@Temperature -40.0 °F |
ASTM D1043 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -46.7 °C | -52.1 °F | ASTM D746 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 3.0 % <br>@Thickness 1.91 mm |
3.0 % <br>@Thickness 0.0750 in |
ASTM D1003 |
| Transmission, Visible | 85 % <br>@Thickness 1.91 mm |
85 % <br>@Thickness 0.0750 in |
ASTM D1003 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
| 188 - 199 °C | 370 - 390 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Clear/Transparent | |
| Features | High Gloss | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Hose | |
| Tubing |