Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 343 - 391 °C | 649 - 736 °F | |
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boil.. |
|||
Melt Temperature | 343 - 391 °C | 649 - 736 °F | |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn.. |
|||
Melt Temperature | 343 - 399 °C | 649 - 750 °F | |
Solvay Specialty Polymers Udel® GF-130 Polysulfone (PSU)
(Unverified Data**) Udel GF-130, resin is a 30% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi.. |
|||
Melt Temperature | 343 - 349 °C | 649 - 660 °F | |
Solvay Specialty Polymers PrimoSpire® PR-250 Polyphenylene, Self-Reinforced (SRP) PrimoSpire® PR-250 resin is an injection molding grade of self-reinforced polyphenylene (SRP). PrimoSpire® SRP is an ultra-high performance amorphous, melt-processable polymer. The unique prop.. |
|||
Melt Temperature | 343 - 388 °C | 649 - 730 °F | |
Solvay Specialty Polymers Radel® R-5100 Polyphenylsulfone (PPSU), Filled Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, h.. |
|||
Melt Temperature | 343 - 399 °C | 649 - 750 °F | |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU), Glass Fiber Udel® GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical res.. |
|||
Melt Temperature | 343 - 399 °C | 649 - 750 °F | |
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU), Glass Fiber Udel® GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical .. |
|||
Melt Temperature | 343 - 399 °C | 649 - 750 °F | |
Solvay Specialty Polymers Udel® GF-130 Polysulfone (PSU), Glass Fiber Udel® GF-130, resin is a 30% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical .. |
|||
Melt Temperature | 343 - 385 °C | 649 - 725 °F | |
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU) Veradel® 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, .. |
|||
Melt Temperature | 343 - 385 °C | 649 - 725 °F | |
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
Melt Temperature | 343 - 385 °C | 649 - 725 °F | |
Solvay Specialty Polymers Veradel® 3300 ULT Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability as well as resistance to steam, hot water and mineral a.. |
|||
Melt Temperature | 343 - 399 °C | 649 - 750 °F | |
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU), 30% Glass Fiber Veradel® 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Melt Temperature | 343 - 399 °C | 649 - 750 °F | |
Solvay Specialty Polymers Veradel® 3430GF Polyethersulfone (PESU), 30% Glass Fiber Veradel® 3430GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Melt Temperature | 343 - 385 °C | 649 - 725 °F | |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
Melt Temperature | 343 - 385 °C | 649 - 725 °F | |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU) Veradel® 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to s.. |
|||
Melt Temperature | 343 - 385 °C | 649 - 725 °F | |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci.. |
|||
Melt Temperature | 343 - 399 °C | 649 - 750 °F | |
Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU), 20% Glass Fiber Veradel® AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Melt Temperature | 343 - 399 °C | 649 - 750 °F | |
Solvay Specialty Polymers Veradel® AG-330 Polyethersulfone (PESU), 30% Glass Fiber Veradel® AG-330 is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Melt Temperature | 343 - 377 °C | 649 - 711 °F | Stock |
PolyOne Stat-Tech™ RA-06CF-07GF/000 EM Polyarylsulfone - 7% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications - Flow Enhanced Grade Data provided by PolyOne. |
|||
Melt Temperature | 343 - 377 °C | 649 - 711 °F | Stock |
PolyOne Stat-Tech™ RA-06CF-09GF/000 Polyarylsulfone - 9% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications
&a Data provided by PolyOne. |
|||
Melt Temperature | 343 - 399 °C | 649 - 750 °F | Average value: 365 °C Grade Count:12 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Melt Temperature | 343 - 371 °C | 649 - 700 °F | Stock |
PolyOne Edgetek® CTXC-084 Polyethersulfone - Mineral Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 343 - 385 °C | 649 - 725 °F | |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensional sta.. |
|||
Melt Temperature | 343 - 391 °C | 649 - 736 °F | |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensional sta.. |
|||
Melt Temperature | 343 - 385 °C | 649 - 725 °F | |
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and .. |
|||
Melt Temperature | 343 - 399 °C | 649 - 750 °F | |
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU)
(Unverified Data**) Veradel 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Melt Temperature | 343 - 385 °C | 649 - 725 °F | |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. .. |
|||
Melt Temperature | 343 - 391 °C | 649 - 736 °F | |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. .. |
|||
Melt Temperature | 343 - 399 °C | 649 - 750 °F | |
Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU)
(Unverified Data**) Veradel AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Melt Temperature | 343 - 385 °C | 649 - 725 °F | |
Solvay Specialty Polymers Veradel® 3300 Polyethersulfone (PESU)
(discontinued **) Veradel 3300 polyethersulfone (PESU) is a medium melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, b.. |