Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 260 - 270 °C | 500 - 518 °F | |
Polyplastic Armamid® PA GF50-1 Nylon 6, 50% Glass Fiber High stiffnessInformation provided by PolyPlastic Group. |
|||
Melt Temperature | 260 °C | 500 °F | |
Chevron Phillips 6120 LLDPE Cast/Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applicationsAp.. |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | DAM |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) Zytel® EFE7374 is a 40% fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for injection molding. It has an improved impact resistance and excellent surface appearance and gloss.I.. |
|||
Melt Temperature | 260 - 310 °C | 500 - 590 °F | |
Akro-Plastic Akromid® S31 (3484) PA 6.10 Dry
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Melt Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical Lupox® TE5000D PBT+PC Description: Injection Molding, PBT+PC, Good SurfaceApplication: E&E, Automotive (Lamp Housing)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
LG Chemical Lupox® TE-5020 High Impact PBT, Thermoplastic Elastomer Alloy, Blow Molding LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
LG Chemical LUPOY SR3108FC PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
Melt Temperature | 260 °C | 500 °F | for test specimens; ISO 294 |
Lanxess Pocan® B 5220 XF 000000 PBT, 20% Glass Spheres PBT, 20% glass spheres, injection molding, improved flowability, improved impact strength, low tendency to warpInformation provided by LANXESS. |
|||
Melt Temperature | 260 °C | 500 °F | Injection Molding; ISO 294 |
Lanxess Pocan® BF 4225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, flame retardant |
|||
Melt Temperature | 260 °C | 500 °F | Injection Molding; ISO 294 |
Lanxess Pocan® DP BF 4232 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Melt Temperature | <= 260 °C | <= 500 °F | |
Total PS CPDS 818E Flame Retardant Polystyrene POLYSTYRENE (PS) COMPOUND (CPDS) 818E is a high impact brominated flame retardant polystyrene. A combination of high flow and high heat stability gives excellent processability and reduced cycle ti.. |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
A. Schulman ComAlloy® E-12672 Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
A. Schulman VOLOY™ 462 Hybrid Reinforced PBT Alloy Information provided by A. Schulman. |
|||
Melt Temperature | 260 - 282 °C | 500 - 540 °F | |
Eastman Tritan MX810 Copolyester Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceOutstanding impact re.. |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | ISBM |
Eastman Tritan TX1800 Copolyester Applications:Consumer and durable goodsExtrusion blow moldingInjection stretch blow moldingKey Attributes:Ease of processingExcellent clarityExcellent Hydrolytic stabilityGood chemical resistanceGoo.. |
|||
Melt Temperature | 260 °C | 500 °F | Injection molding; ISO 294 |
Covestro Bayblend® ET3032 FR Rubber Modified PC Blend, 10% Mineral Filled Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend.. |
|||
Melt Temperature | 260 °C | 500 °F | Injection Molding; ISO 294 |
Covestro Bayblend® KU 2-1514 BBS073* Polycarbonate + ABS, Flame Retardant Grade Developmental productHigh heat resistant injection molding gradeimproved chemical resistance and stress cracking behavior compared to KU 2-1514ball indentation temperature = 125 °CVicat/B 120 tempe.. |
|||
Melt Temperature | 260 - 290 °C | 500 - 554 °F | |
CP-Polymer-Technik Wellamid® 6000 MRGV 20/10 HWCP 20% Mineral and 10% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
CP-Polymer-Technik Wellamid® 6600/42 HWCP Nylon 66, Polymer Modified, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
CP-Polymer-Technik Wellamid® 6600/506 HWCP Nylon 66, Impact Modified, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
CP-Polymer-Technik Wellamid® 6600/508 HWUVCP Nylon 66, Impact Modified, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
Covestro Makroblend® DP 2-7655 MBS162 Polycarbonate + PET, Mineral Filled Impact Grade Developmental product(PC+PET)-blendsimpact modifiedInjection molding grade 10% mineral filledAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new .. |
|||
Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
Covestro Makroblend® DP 2-7655 Polycarbonate + PET, Mineral Filled Impact Grade Developmental productISO 7792-1-PC/PET,MHPR,-030,MD10(PC+PET)-blendsimpact modifiedInjection molding grade 10% mineral filledPreprocessingMax. Water content |
|||
Melt Temperature | 260 °C | 500 °F | Injection Molding; ISO 294 |
Lanxess Pocan® B 3215 000000 PBT, 10% Glass Fiber PBT, 10% glass fibers, injection molding |