Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 182 - 199 °C | 360 - 390 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion L7703 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Flexible A65M0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Flexible B85B0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Flexible R130AE White 41 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | |
PolyOne Geon™ Vinyl Flexible R5145B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Flexible XV3878G Polyvinyl Chloride + NBR (PVC+NBR) Information provided by PolyOne |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | |
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | |
PolyOne Geon™ Vinyl Flexible B550B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Flexible C70A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 199 °C | 379 - 390 °F | |
PolyOne Geon™ Vinyl Flexible C70T0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 199 °C | 379 - 390 °F | |
PolyOne Geon™ Vinyl Flexible C70U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Flexible R158AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Flexible R5257A White 759 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | with BUR of 1.5:1 or higher |
Westlake EF412 Low Density Polyethylene WESTLAKE polyethylene EF412 is a low-density polyethylene with very good optical and strength properties. This material is an excellent choice for bakery films and food packaging applications.Applic.. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | with BUR of 1.5:1 or higher |
Westlake Elevate™ EF437 2.5% Ethylene Vinyl Acetate Copolymer Westlake EF437 resin is a 2.5% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low.. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | with BUR of 1.5:1 or higher |
Westlake Elevate™ EF439 4.0% Ethylene Vinyl Acetate Copolymer Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio.. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | with BUR of 1.5:1 or higher |
Westlake EP310 Low Density Polyethylene WESTLAKE polyethylene EP310 is a low-density polyethylene suggested for cast film bakery applications. This material has outstanding optical and processing properties.Application/UsesBakery bagsSoft.. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | with BUR of 1.5:1 or higher |
Westlake EP413 Low Density Polyethylene WESTLAKE polyethylene EP413 is a low-density polyethylene recommended for blown or cast film clarity applications. This material has very good optical properties, and is suggested for bakery films ,.. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | Extrusion |
Total HDPE BM962 High Density Polyethylene, High Gloss Blow Molding Resin Polyethylene: High density High Gloss Blow Molding ResinCharacteristics:High GlossHigh stiffnessGood abrasion resistanceFDA CompliantApplications:Coextruded glossy bottlesBlending agent for other p.. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | Extrusion |
Lubrizol Estane® 2103-80AE Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | Extrusion |
Lubrizol Estane® 2103-84AEN Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Contains UV Stabilizer, NSF Standard 61 certifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pelletha.. |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
Axiall HHW-191 Rigid PVC, Extrusion Georgia Gulf HHW-191 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Excellent WeatherabilityImpact Strength & ToughnessColorabilityChemic.. |
|||
Melt Temperature | 188 - 199 °C | 370 - 390 °F | |
PolyOne Geon™ Vinyl Flexible A55G0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 182 - 199 °C | 360 - 390 °F | |
M. Holland Company MAGMA® LM233-A LLDPE
(discontinued **) Features: Good Heat Seal, Good ProcessabilityUses: Coating Applications, Film, Cast Film, PackagingProcessing Method: Coextrusion, Blown FilmInformation provided by M. Holland. |