Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Melt Temperature | 225 °C | 437 °F | Optimum; Extrusion |
DuPont Performance Polymers Hytrel® 5553FG NC010 TPC-ET
(Unverified Data**) Hytrel® 5553FG NC010 is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont |
|||
Melt Temperature | 225 - 235 °C | 437 - 455 °F | |
NOVA Chemicals Sclair® 14B3 Butene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |
|||
Melt Temperature | 225 - 310 °C | 437 - 590 °F | Average value: 269 °C Grade Count:6 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Melt Temperature | 225 - 310 °C | 437 - 590 °F | Average value: 272 °C Grade Count:13 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Melt Temperature | 225 - 320 °C | 437 - 608 °F | Average value: 288 °C Grade Count:5 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Melt Temperature | 225 °C | 437 °F | LCL-PR29 |
Intercontinental Polymers HoPBT 303 HoPBT Polymer Type - Clear, Polyester Pellets Applications: Engineering Resin Information provided by Intercontinental Polymers. |
|||
Melt Temperature | 225 °C | 437 °F | |
Iran Petrochemical (PCC) LL0209 KJ Linear Low Density Polyethylene LL 0209 is a LLDPE copolymer with butene as comonomer which contains anti-oxidant, Slip and antiblock additives. It gives film of high slip which is easily separable. It is recommended for general .. |
|||
Melt Temperature | 225 °C | 437 °F | |
SIDPEC EGYPTENE® LL 0209 KJ LLDPE Film Applications:Refuse sacksProduce bags, carrier bagsFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
Melt Temperature | 225 °C | 437 °F | |
SIDPEC EGYPTENE® LL 0220 AA LLDPE Film Applications:Light and medium duty filmStretch filmFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
Melt Temperature | 225 °C | 437 °F | |
SIDPEC EGYPTENE® LL 0205 AF LLDPE Film Applications:Heavy duty sacks, mulch filmsStretch film, liners, geomembraneFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l... |
|||
Melt Temperature | 225 - 260 °C | 437 - 500 °F | |
Eastman Ecdel PCCE 9967 Copolyester Ether Elastomer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Melt Temperature | 225 - 235 °C | 437 - 455 °F | |
Covestro Desmopan® 481 Polyurethane injection molding gradefree from plasticizersgrease and oil-resistantlow compression sethigh elasticitygood heat resistanceEasy releaseApplicationRoller coatingSealsmembranesAutomotive engineeringPr.. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen HU 70E3 HDPE, Injection Molding Starpylen HU 70E3 is a High Density Polypropylene Injection Molding Resin (also known as HU70E3)Information provided by Eurostar. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen HZ 50E3 PP, Injection Molded PRELIMINARY-Starpylen HZ 50E3 is a High Specific Gravity Polypropylene (density 1.5), Injection Molding Resin (also known as HZ50E3)Information provided by Eurostar. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen HZ 80E7 HDPE, Injection Molding Starpylen HZ 80E7 is a High Specific Gravity Polypropylene, Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MF007AS PP, Glass Fiber Filled, Injection Molded Starpylen MF007AS is a Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MX05038 TPEX, Injection Molded Starpylen MX05038 is a TPEX Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MX06023 PP, 20% Milled Glass Fiber Filled, Injection Molded Starpylen MX06023 is a 20% Milled Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Ultramid® HFX 33 PA6 (Dry) Description: Ultramid HFX 33 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en.. |
|||
Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Ultramid® HFX 35 PA6 (Dry) Description: Ultramid HFX 35 is a polyamide specialty extrusion resin combining high flexibility, outstanding chemical resistance and enhanced heat stability.Applications: Ultramid HFX 35 is recomme.. |
|||
Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
Beijing Ranger Chem PBT-201-G0 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
Beijing Ranger Chem PBT-201-G10 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Beijing Ranger Chem PBT-201-G30 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Beijing Ranger Chem PBT-201-G20 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Beijing Ranger Chem PBT-201-G30 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Temperature | 225 °C | 437 °F | |
Formosa Plastics Formolene® L62005E2T1 Film (Hexene Grade) LLDPE
(discontinued **) Hexene Copolymer (High slip and antiblock, with processing aid)Applications: Blown film, high strength applicationsBlown film, high strength applicationsMeets all requirements of the U.S. Food and D.. |
|||
Melt Temperature | 225 - 235 °C | 437 - 455 °F | |
NOVA Chemicals Sclair® 14B1 Butene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |
|||
Melt Temperature | 225 °C | 437 °F | Optimum; Injection Molding |
DuPont Performance Polymers Hytrel® 4068FG TPC-ET
(Unverified Data**) Hytrel® 4068FG is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont Performance Polymers |