Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PP CCP20020 UV Polypropylene, Mineral Reinforced, UV stabilized
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PP HIP16020FCF Polypropylene, Fast Cycle
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPC K20040 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPC T25020 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPC TS20020 UV Polypropylene Copolymer, Mineral Reinforced, UV-Stabilized
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPH GF15020 PD1 NBR PP, Glass Fiber-Reinforced, Chemically Coupled
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPH GF5015 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPH GF5030 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPH TS15020 D Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPHC K2040H Polypropylene, Mineral Reinforced
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPC B10075 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPC BGK601213 CR Polypropylene Copolymer, Multifiller
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPC GF15030 PD2 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPH B8075 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPH GF8030 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPH GF8030 PD1 VT2 PP, Glass Fiber-Reinforced, Chemically Coupled Heat Stabilized
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPH T20020 UV Polypropylene Homopolymer, Mineral Reinforced, UV-Stabilized
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPH T4060 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Melt Temperature |
205 - 245 °C |
401 - 473 °F |
|
Huntsman Rexell® V8801 Cast Film Extrusion LLDPE
(discontinued **)
Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |
Melt Temperature |
205 °C |
401 °F |
Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 988PA NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® 988PA NC010 is a low viscosity acetal homopolymer for injection molding with low screw deposit. It is especially formulated for gear applications requiring high precision and dimensional st.. |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Ineos ABS Lustran® SAN Sparkle Highest-Clarity
|
Melt Temperature |
205 - 245 °C |
401 - 473 °F |
|
Huntsman Rexell® L8404 Cast Film Extrusion LLDPE
(discontinued **)
Linear-low density copolymer, and FDA compliant.Applications: Blown film extrusion: general purpose.Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1.Information provided by H.. |
Melt Temperature |
205 - 245 °C |
401 - 473 °F |
|
Huntsman Rexell® L8408 Cast Film Extrusion LLDPE
(discontinued **)
Linear-low density copolymer, high quality blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength optics, and very low gel levels.Applications: Seali.. |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPH FX801020 Polypropylene Homopolymer, Glass Reinforced
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPH GF10020 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPH TS15010 H VTUV1 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPH TS4040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPH TS5040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPH TS8030 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Melt Temperature |
205 - 260 °C |
401 - 500 °F |
|
Polykemi AB POLYfill PPHC K8040G E10 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB |