Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Filler Content 25 %
25 %
±2%; Polykemi
Linear Mold Shrinkage 0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
With Flow; ISO 2577
0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
Across Flow; ISO 2577
Melt Index of Compound 6.0 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
6.0 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 18.0 MPa
<= 2610 psi
ISO/R527
Elongation at Yield 9.0 %
9.0 %
ISO/R527
Flexural Strength <= 43.0 MPa
<= 6240 psi
ISO 178
Flexural Modulus 1.60 GPa
<br>@Temperature 23.0 °C
232 ksi
<br>@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.500 J/cm²
<br>@Temperature -20.0 °C
2.38 ft-lb/in²
<br>@Temperature -4.00 °F
ISO 179
1.50 J/cm²
<br>@Temperature 23.0 °C
7.14 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
120°C/h; ISO 75/1
Vicat Softening Point 83.0 °C
<br>@Load 5.001 kg
181 °F
<br>@Load 11.03 lb
50°C/h; ISO 306
145 °C
<br>@Load 1.00 kg
293 °F
<br>@Load 2.21 lb
50°C/h; ISO 306
Flammability, UL94 HB
<br>@Thickness 1.60 mm
HB
<br>@Thickness 0.0630 in
Processing Properties Metric English Comments
Melt Temperature 205 - 260 °C
401 - 500 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Dry Time 2 - 4 hour
2 - 4 hour
in circulation dryer
2 - 4 hour
2 - 4 hour
in desiccant air dryer
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Back Pressure 1.00 - 2.00 MPa
145 - 290 psi
Descriptive Properties Value Comments
Holding Pressure () 20-40
% of injection pressure
Injection Speed () High