Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 12.0 Month | 12.0 Month | |
NBE nanoTach® Nano-Silver Paste, Lead-Free Solder Alternative NanoTach® is a thick paste of nano-sized silver powder in an organic binder that can be used as an alternative to solder or epoxy in semiconductor devices in the state-of-the-art individual package.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | Normal Storing Conditions |
Premix Thermoplastics PRE-ELEC® PE 1271 PRE-ELEC PE 1271 is a conductive thermoplastic compound based on a blend of PE-LD/PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivi.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | Normal Storing Conditions |
Premix Thermoplastics PRETHERM TPE 1075 Thermoplastic Elastomer, Boron Nitride / SEBS compound PRETHERM TPE 1075 is a thermoplastic elastomer based highly thermally conductive compound intended primarily for heat dissipation. It can be used as gap filler between processor and heat sink or co-.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | Normal Storing Conditions |
Premix Thermoplastics PREWHITE PE 20-50 PREWHITE PE 20-50 is a PE-LLD based white masterbatch, developed for PE-LD, PE-LLD and PE-HD films, injection and blow molded products. PREWHITE PE 20-50 can also be used in blown films at high mast.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | under dry and cool conditions |
TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber Millathane 28 has excellent resistance to gas (e.g., nitrogen) permeability as well as very good abrasion resistance and low temperature properties. This polyurethane rubber was designed for automot.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Permabond 930 Cyanoacrylate PERMABOND 930 is a low odor, nonfogging, nonfrosting cyanoacrylate. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The .. |
|||
Shelf Life | 12.0 Month @Temperature 5.00 - 10.0 °C |
12.0 Month @Temperature 41.0 - 50.0 °F |
in unopened original container |
Heraeus Cleviosâ„¢ P VP CH 8000 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P VP CH 8000 is an antistatic material based o.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Solvay MIRACARE® SLB-205/N Surfactant Description: Miracare SLB-205/N is a free flowing, high active surfactant concentrate used in the preparation of structured liquids. It is a surfactant base used to stabilize additives applied in a .. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Solvay MIRAPOL® 550 P Surfactant Description: Mirapol 550 P can be used effectively in shampoos and conditioners at typical use levels of 0.5% (copolymer solids) to provide excellent lubricity, softeness light hair conditioning and.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | unopened containers |
Master Bond EP112 Low Viscosity Heat Curing Cycloaliphatic Epoxy Adhesive Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical & e.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Dow Corning SLYGARD® 527 A&B SILICONE DIELECTRIC GEL Two-parts, clear, RT or heat cure.Information provided by Dow Corning |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Dow Corning SYL-OFF® SL 8 CROSSLINKER Solvent-free, fast curing, actively reduces mist at high speeds, good balance of cure and anchorage performanceInformation provided by Dow Corning |
|||
Shelf Life | 12.0 Month @Temperature -40.0 °C |
12.0 Month @Temperature -40.0 °F |
|
Epoxy Technology EPO-TEK® E3001-HV Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E3001-HV is a snap cure, single component, silver-filled die attach adhesive for semiconductor plastic IC packaging. Also available in a frozen syringe. Advantages & .. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Dow Corning 236 DISPERSION Flowable (as supplied) silicone RTV coatingInformation provided by Dow Corning |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Dow Corning 3-4170 DIELECTRIC GEL KIT Two-part, clear, heat cure, long working time.Information provided by Dow Corning |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Dow Corning 3-4222 DIELECTRIC FIRM GEL KIT Two-part, translucent green, firm, fast RT or heat cure, and primerless chemical adhesion.Information provided by Dow Corning |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Dow Corning 3730 A&B KIT A 2 part solventless and colourless liquid silicone rubber with particularly good adhesion to polyamide as well as glass fabric. Cured rubber coating is high strength and has high elongationInformat.. |
|||
Shelf Life | 12.0 Month @Temperature 4.00 - 38.0 °C |
12.0 Month @Temperature 39.2 - 100 °F |
0-95% RH |
3M 4298UV Adhesion Promoter 3M™ Adhesion Promoter 4298UV is a liquid primer used to improve the adhesion of 3M™ Acrylic Foam Tapes to low surface energy plastics such as thermoplastic olefins (TPO), thermoplastic urethanes (.. |
|||
Shelf Life | 12.0 Month @Temperature 21.1 °C |
12.0 Month @Temperature 70.0 °F |
|
Arlon I51576R015 Silicone Rubber/Fiberglass/Alloy Laminate Top layer of side 2: alloy 600 foil; Bottom layer of side 2: cured silicone rubber; Substrate is 7628 fiberglass; Side 1: cured silicone rubber |
|||
Shelf Life | 12.0 Month @Temperature 21.1 °C |
12.0 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon R34172W008 0.008" (0.203 mm) Cured, Unsupported Silicone Rubber on a Mylar Carrier Design/Construction:Side 1: Cured, Unsupported Silicone Rubber on a Mylar Carrier This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Shelf Life | 12.0 Month @Temperature 21.1 °C |
12.0 Month @Temperature 70.0 °F |
|
Arlon T4020-R002 0.020" Cured, Fusible Silicone Rubber with Fiberglass Substrate 0.5 inch wide, 20 mil thick, red, rectangular cross-section, fusible silicone tape.Design/Construction:Side 1: Cured Fusible Silicone RubberSubstrate: 15% Sinusoidal FiberglassSide 2: Cured Fusibl.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | 10-25°C |
Amity Thermosets ATG 115 Phenolic Molding Organic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic .. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Aremco Ceramacast™ 510 High Temperature Potting & Casting Material Alumina Coarse grain castable for producing large hi-temp tooling. |
|||
Shelf Life | 12.0 Month @Temperature 21.1 °C |
12.0 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon 910-10W##-P0 0.010" (0.254 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 10 mil thick, White, Rectangular cross-section, Self-fu.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | in the original unopened package |
3M Novec™ 2704 Electronic Grade Coating 3M™ Novec™ 2704 Electronic Grade Coating is designed for the protection of printed circuit boards and electronic components. It is a clear, low viscosity solution of a 4 wt% fluoropolymer carried .. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Permabond ET514 Epoxy Resin PERMABOND ET514 is a 1:1 mixable epoxy adhesive. It has excellent resistance to impact and vibration and is ideal for structural bonding of metal, wood, composites and certain plastics. Its rapid cu.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Solvay RHODAFAC® RS-410 Surfactant Identification: Phosphate Esters, Branched Alcohol Ethoxylate basedCAS: 9046-01-9Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODAFAC RS-410 very effective APE F.. |