| Category | Polymer , Adhesive , Thermoset , Silicone |
| Manufacturer | Dow Corning |
| Trade Name | SLYGARD® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Dow Corning SLYGARD® 527 A&B SILICONE DIELECTRIC GEL.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.950 g/cc @Temperature 25.0 °C |
0.950 g/cc @Temperature 77.0 °F |
|
| Viscosity | 430 cP | 430 cP | dynamic |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
| Minimum Service Temperature, Air | -45.0 °C | -49.0 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | |
| Dielectric Constant | 2.85 @Frequency 100 Hz |
2.85 @Frequency 100 Hz |
|
| 2.85 @Frequency 100000 Hz |
2.85 @Frequency 100000 Hz |
||
| Dielectric Strength | 15.2 kV/mm | 385 kV/in | |
| Dissipation Factor | 0.00010 @Frequency 100000 Hz |
0.00010 @Frequency 100000 Hz |
|
| 0.0020 @Frequency 100 Hz |
0.0020 @Frequency 100 Hz |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 1440 - 10100 min @Temperature 22.0 °C |
24.0 - 168 hour @Temperature 71.6 °F |
|
| Shelf Life | 12.0 Month | 12.0 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | clear | |
| Color | red | |
| Flowable | yes | |
| Gel Hardness (Grams/Penetration) | 115 | |
| Hydrophobic | yes | |
| Self Leveling | yes | |
| Water Resistant | yes | |
| Working Time (min) | 90 |