Material Notes:
PERMABOND ET514 is a 1:1 mixable epoxy adhesive. It has excellent resistance to impact and vibration and is ideal for structural bonding of metal, wood, composites and certain plastics. Its rapid cure speed coupled with its structural strength makes this adhesive suitable for a wide variety of applications. ET514 is high strength and has excellent environmental durability. Features & Benefits: Adhesion to a wide variety of substrates Rapid cure at room temperature Easy to apply High shear and peel strength Good impact strength Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ET514A, Epoxy Resin
1.21 g/cc
1.21 g/cc
ET514B, Polyamine Hardener
Viscosity 60000 - 70000 cP

@Temperature 25.0 °C
60000 - 70000 cP

@Temperature 77.0 °F
ET514A, Epoxy Resin
70000 - 80000 cP

@Temperature 25.0 °C
70000 - 80000 cP

@Temperature 77.0 °F
ET514B, Polyamine Hardener
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 68 - 72
68 - 72
Elongation at Break 15 - 20 %
15 - 20 %
Adhesive Bond Strength 18.0 - 20.0 MPa
2610 - 2900 psi
Mild steel, Shear
Peel Strength 1.80 - 2.40 kN/m
10.3 - 13.7 pli
ISO 4578
Thermal Properties Metric English Comments
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg 40.0 °C
104 °F
Processing Properties Metric English Comments
Cure Time 40.0 - 60.0 min
0.667 - 1.00 hour
handling time
1440 min
24.0 hour
full cure
Pot Life 30.0 - 40.0 min

@Temperature 20.0 °C
30.0 - 40.0 min

@Temperature 68.0 °F
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Black for Polyamine Hardener
White for Epoxy Resin
Maximum Gap Fill (mm) 2
Strength Retention 10% at 150°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 100°C
Relative to 0°C
93% at 50°C
Relative to 0°C