Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 60.0 Month @Temperature 23.9 °C |
60.0 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon 5163X0085 0.0085" (0.216 mm) Cured Silicone Rubber with Fiberglass Substrate
(discontinued **) 50 inches Overall Width. Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone RubberProduct Description: Acoustical dampeningAppearance: Silver silicone on fiberglass clothThis d.. |
|||
Shelf Life | 60.0 Month @Temperature 21.1 °C |
60.0 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon R3313X016-38 0.0165" (0.419 mm) Cured Silicone Rubber with Fiberglass Substrate 38" Wide
(dis Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning 702 DIFFUSION PUMP FLUID A clear, mixed phenylmethyl dimethyl cyclosiloxane fluid designed for fast pumping of large volumes of gas down from 10-5 to 10-7. Also used on vapor ejector pumps that attain vacuums of 10-4 to 10-.. |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning 705 DIFFUSION PUMP FLUID A colorless, penta phenyltrisiloxane, single-component fluid designed for ultrahigh vacuums of 10-10 torr (untrapped) and 10-11 (trapped).Information provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning MOLYKOTE® 1292 LONG LIFE BEARING GREASE For high-temperature use and applications that come in contact with solvents, fuels and water; recommended for rolling element and plain bearings. Light consistency; resists solvents, fuels and moi.. |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning MOLYKOTE® 3451 CHEMICAL RESISTANT BEARING GREASE Fluorosilicone grease thickened with PTFEInformation provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning MOLYKOTE® 41 HIGH TEMPERATURE BEARING GREASE Phenyl-methyl silicone grease thickened with carbon blackInformation provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning MOLYKOTE® 55 O-RING GREASE Phenyl-methyl silicone grease formulated for O-ringsInformation provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning MOLYKOTE® G 68 Semi-synthetic greaseInformation provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning MOLYKOTE® G-0052 FG WHITE EP BEARING GREASE Aluminum complex-thickened mineral oil food grade greaseInformation provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning MOLYKOTE® PG-21 PLASTISLIP GREASE Silicone grease especially for plastic/plastic and plastic/metal combinations like control cables and circuit lever systemInformation provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning Z-1229 TETRACHLOROSILANE Fiber optic gradeInformation provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning XIAMETER® PMCPPMX-0210 Silicone Fluid 100CS Is chemically equivalent to DOW CORNING® 210H FLUID 100CS. This product is a heat stabilized polydimethlysiloxane, used for heat transfer.Information provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning Z-1224 TRIMETHYLCHLOROSILANE Information provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning 340 Heat Sink Compound White, non-flowing, highly filled compound, good thermal conductivity.Information provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning 4 ELECTRICAL INSULATING COMPOUND Silicone-based compound, moderate consistency. Lubricant suitable for electrical connectors and joints.Information provided by Dow Corning |
|||
Shelf Life | 60.0 Month @Temperature 21.1 °C |
60.0 Month @Temperature 70.0 °F |
|
Arlon 26122P020 0.020" Cured Silicone Rubber/Laminated PTFE Film Design/Construction:Interleave: 0.002" ETFESide 1: Cured Silicone RubberLaminated Substrate: Cast PTFE FilmThis data represents typical values for the production material and should not be used a.. |
|||
Shelf Life | 60.0 Month @Temperature 21.1 °C |
60.0 Month @Temperature 70.0 °F |
|
Arlon 55572GA028 0.028" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material .. |
|||
Shelf Life | 60.0 Month @Temperature 21.1 °C |
60.0 Month @Temperature 70.0 °F |
|
Arlon 99322B015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Static dissipating siliconeDesign/Construction:Interleave: 0.0025" PolyethyleneSide 1: Cured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Chemlock 607This data repres.. |
|||
Shelf Life | 60.0 Month @Temperature 23.9 °C |
60.0 Month @Temperature 75.0 °F |
|
Arlon R35232B050 0.050" Fully Cured, Static Dissipating Silicone Rubber Fully cured, unsupported, static dissipating silicone.Design/Construction:Liner: 3 mil PolyethyleneProduct: Fully Cured Silicone RubberCarrier: N/AThis data represents typical values for the produc.. |
|||
Shelf Life | 60.0 Month @Temperature 23.9 °C |
60.0 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon R37292S018 0.018" (0.457 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberCarrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be used .. |
|||
Shelf Life | 60.0 Month @Temperature 23.0 °C |
60.0 Month @Temperature 73.4 °F |
From date of manufacture |
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628.. |
|||
Shelf Life | 60.0 Month @Temperature 22.8 °C |
60.0 Month @Temperature 73.0 °F |
|
Arlon UltraPad™ 51073G031D Silicone-Based Press Pad Green UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data.. |
|||
Shelf Life | 60.0 Month @Temperature 23.9 °C |
60.0 Month @Temperature 75.0 °F |
|
Arlon 51163X0085 0.0085" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone Rubber50" wideThis data represents typical values for the production material and should not.. |
|||
Shelf Life | 60.0 Month @Temperature 21.1 °C |
60.0 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon 55272R028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
Shelf Life | 60.0 Month @Temperature 21.1 °C |
60.0 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon 99202R008 0.008" (0.203 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Interleave: FEP FilmSide 1: Cured Silicone Rubber Carrier: PTFE Coated FiberglassProduct Use: Adhesive. Bonds without primer.Appearance: Off-white, High viscosity gum on release.. |
|||
Shelf Life | 60.0 Month @Temperature 21.1 - 26.7 °C |
60.0 Month @Temperature 70.0 - 80.0 °F |
From date of manufacture |
Arlon R35232B085 0.085" (2.16 mm) Fully Cured Silicone Rubber Description: Fully cured, unsupported, static dissipation siliconeDesign/Construction:Liner: Polyethylene Product: Fully Cured Silicone RubberAppearance: Black cured siliconeThis data represents typ.. |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
3M Novec™ Contact Cleaner 3M™ Novec™ Contact Cleaner effectively removes light oils, greases, silicones, dust and particulates from sensitive electrical and electronic equipment. Meets MIL-PRF 29608A Class C specifications.. |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
3M Novec™ Electronic Degreaser 3M™ Novec™ Electronic Degreaser is a strong non-flammable cleaner ideal for removal of heavy oils, greases and handling soils from internal components of electronic equipment, precision devices an.. |
|||
Shelf Life | 60.0 Month @Temperature 23.9 °C |
60.0 Month @Temperature 75.0 °F |
|
Arlon R37582R0055 0.0055" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassThis data represents typical values for the production material and should not be .. |