Arlon R35232B085 0.085" (2.16 mm) Fully Cured Silicone Rubber

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R35232B085 0.085" (2.16 mm) Fully Cured Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Fully cured, unsupported, static dissipation siliconeDesign/Construction:Liner: Polyethylene Product: Fully Cured Silicone RubberAppearance: Black cured siliconeThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Liner
2160 microns
85.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength 4.83 MPa
700 psi
ASTM D412
Elongation at Break 290 %
290 %
ASTM D412
Compression Set 25 %
25 %
Arlon SQA-TMS-017
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 - 26.7 °C
60.0 Month

@Temperature 70.0 - 80.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Black
Total Product Weight (oz/yd2) 75.6