Material Notes:
Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberCarrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 457 microns
18.0 mil
Overall; Arlon SQA-TMS-003
457 microns
18.0 mil
Side 1; Arlon SQA-TMS-003
457 microns
18.0 mil
Interleave
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Silicone Property; ASTM D2240
Tensile Strength 8.62 MPa
1250 psi
Silicone Property; ASTM D412
Elongation at Break 800 %
800 %
Silicone Property; ASTM D412
Tear Strength 38.6 kN/m
220 pli
Die B, Silicone Property; ASTM D624
Compression Set 19 %
19 %
Arlon SQA-TMS-017
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 50.20 kV/mm
1275 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 60.0 Month

@Temperature 23.9 °C
60.0 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Saddle Brown
Total Product Weight (oz/yd2) 15.1
Arlon SQA-TMS-025