Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name Thermabond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material. The data should not be used to write, or in place of, material specificationsInformation provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 2.80 g/cc
0.101 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 63.5 microns
2.50 mil
Liner
102 microns
4.00 mil
Side 1; Arlon SQA-TMS-003
203 microns
8.00 mil
Substrate; Arlon SQA-TMS-003
305 microns
12.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
Silicone Property; ASTM D2240
Tensile Strength 4.72 MPa
685 psi
Silicone Property; ASTM D412
Tensile Strength, Yield 24.5 MPa

@Strain <=1.00 %
3550 psi

@Strain <=1.00 %
Arlon SQA-TMS-008
Elongation at Break 125 %
125 %
Silicone Property; ASTM D412
Poissons Ratio 0.50
0.50
Approximately, Silicone Property
Thermal Properties Metric English Comments
CTE, linear 105 µm/m-°C

@Temperature 20.0 - 160 °C
58.3 µin/in-°F

@Temperature 68.0 - 320 °F
Silicone Property; ASTM E 831
Specific Heat Capacity 0.820 J/g-°C

@Temperature 100 °C
0.196 BTU/lb-°F

@Temperature 212 °F
Silicone Property; Arlon SQA-TMS-052
Thermal Conductivity 1.40 W/m-K

@Temperature 100 °C
9.72 BTU-in/hr-ft²-°F

@Temperature 212 °F
Silicone Property; ASTM E 1530
1.50 W/m-K

@Temperature 50.0 °C
10.4 BTU-in/hr-ft²-°F

@Temperature 122 °F
(Apparent), Product Property; ASTM D5470
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Minimum Service Temperature, Air -100 °C
-148 °F
Glass Transition Temp, Tg -118 °C
-180 °F
ASTM D3418
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Dielectric Constant 6.91

@Frequency 1.00e+6 Hz
6.91

@Frequency 1.00e+6 Hz
Silicone Property; IPC TM 650 - 2.5.5.3
Dielectric Strength 27.6 kV/mm
700 kV/in
ASTM D149
Dissipation Factor 0.0044

@Frequency 1.00e+6 Hz
0.0044

@Frequency 1.00e+6 Hz
Silicone Property; IPC TM 650 - 2.5.5.3
Arc Resistance 193 sec
193 sec
ASTM D495-99
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 23.0 °C
60.0 Month

@Temperature 73.4 °F
From date of manufacture
Descriptive Properties Value Comments
Color Gray
Red
Substrate
Total Product Weight (g/m2) 685
Arlon SQA-TMS-025
Users viewing this material also viewed the following: