Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 6.00 Month | 6.00 Month | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 170 LOW ODOR/LOW BLOOM (1500 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 170 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Shelf Life | 6.00 Month @Temperature 4.44 °C |
6.00 Month @Temperature 40.0 °F |
|
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Chopped Molding Compound Reinforced Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz.. |
|||
Shelf Life | 6.00 Month @Temperature 3.00 - 7.00 °C |
6.00 Month @Temperature 37.4 - 44.6 °F |
Chomerics |
Parker Chomerics CHOFORM® 5513 Conductive Form-in-Place Gasket Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Shelf Life | 6.00 Month | 6.00 Month | |
Raschig Group PiMC 1841 Metallic colors Adding metallic effect pigments to powder coatings gave rise to several application problems such as “spitting”. Synres-Almoco’s Metallic PiMC 1841 ensures easy processing and homogeneous surface.. |
|||
Shelf Life | 6.00 Month @Temperature 15.0 - 25.0 °C |
6.00 Month @Temperature 59.0 - 77.0 °F |
|
Raschig Group SURAPLAST UPA 63 UP Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Shelf Life | 6.00 Month @Temperature 25.0 °C |
6.00 Month @Temperature 77.0 °F |
|
Lord Adhesives 8651 Polymer Resistor Composition LORD 8600 series polymer resistor compositions are designed for screen print application onto a wide range of substrates.All information provided by Lord. |
|||
Shelf Life | 6.00 Month | 6.00 Month | |
Gwent Electronic Materials C2091208D1 Carbon Graphite Ink This product is designed to be used for screen printing working electrodes. It gives excellent electrochemical performance with good reversibility when using cyclic voltammetry. The ink should be g.. |
|||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
in original unopened container |
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy Description: Master Bond EP30AN-1 is a two part epoxy for high performance potting, sealing, coating and bonding featuring high thermal conductivity, excellent electrical insulation properties and N.. |
|||
Shelf Life | 6.00 Month | 6.00 Month | At 5°C |
Tra-Con Tra-Duct 921U02 Long Pot Life Silver-Filled Epoxy TRA-DUCT 921U02 long room temperature pot life, silver-filled epoxy. Information provided by Tra-Con Inc. |
|||
Shelf Life | 6.00 Month @Temperature -18.0 °C |
6.00 Month @Temperature -0.400 °F |
|
Hexcel® HexPly® M32 Epoxy Matrix HexPly® M32 is specifically designed for prepreg applications with fabrics and short curing cycles for sporting (e.g. ski and snowboard production) and industrial applications. HexPly® M32 compris.. |
|||
Shelf Life | 6.00 Month | 6.00 Month | |
Dow Corning JCR 6126 W/C Two-part, translucent, thixotropic, medium modulus LED encapsulant with a very long working time.Information provided by Dow Corning |
|||
Shelf Life | 6.00 Month @Temperature 21.1 °C |
6.00 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon 15370P020 0.020" (0.508 mm) Uncured Silicone Rubber on a Mylar Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: MylarAppearance: Pink high viscosity gumThis data represents typical values for the production material. The data.. |
|||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon 32580R035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. .. |
|||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
|
Arlon 49581R010 0.0105" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1681 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the .. |
|||
Shelf Life | 6.00 Month @Temperature 21.1 °C |
6.00 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon 56811B025 0.026" (0.660 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Product Use: Hose and Duct.. |
|||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon R34696R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Shelf Life | 6.00 Month @Temperature -15.0 - -9.44 °C |
6.00 Month @Temperature 5.00 - 15.0 °F |
From date of manufacture |
Arlon R36580N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat.. |
|||
Shelf Life | 6.00 Month | 6.00 Month | |
Atom Adhesives AA-DUCT N02 Epoxy Adhesive AA-DUCT N02 is a single component, heat curing, conductive epoxy polymer that was designed for ease in handling. This high performance conductive polymer cures quickly at elevated temperatures makin.. |
|||
Shelf Life | 6.00 Month | 6.00 Month | |
Aremco Graphi-Coat™ 623 High Temperature Specialty Coatings Inorganic, Titanium Diboride Filled This coating system, originally patented by Aremco, is a tow-part, silica-bonded, titanium diboride filled, oxidation resistant coating for protecting graphite from oxidation to 2000°F (1093°C). U.. |
|||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon 49091R010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data Represents typical values for the production material. The data s.. |
|||
Shelf Life | 6.00 Month @Temperature 21.1 °C |
6.00 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon 49586B010 0.0115" (0.292 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater.. |
|||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
|
Arlon 51561R015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the .. |
|||
Shelf Life | 6.00 Month | 6.00 Month | |
Aremco Pyro-Putty™ 2500 High Temperature Ceramic-Metallic Putty, Iron Oxide Filled Ceramic and Black Iron Oxide-Filled, One-Part, Water Based Paste.For Applications to 1/4" Thick.Repairs Cast Iron, and Steel Parts to 1600°F |
|||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon 44570B010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Layers Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specificati.. |
|||
Shelf Life | 6.00 Month @Temperature 10.0 - 32.0 °C |
6.00 Month @Temperature 50.0 - 89.6 °F |
|
Lord Adhesives Chemlok® Y-1540 Silicone Rubber Adhesive Chemlok® Y-1540 is a one-coat adhesive used to bond peroxide curing silicone, EPDM, and fluoroelastomers to cold rolled and phosphatized steel.All information provided by Lord. |
|||
Shelf Life | 6.00 Month | 6.00 Month | 1 component life at 0ºC |
Loctite® 3880 Heat Cure Isotropic Epoxy Adhesive Electrically Conductive BondersLoctite® Electrically Conductive Adhesives are used in a variety of applications where electrical connectivity is needed, providing a conductive path where traditiona.. |