Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loctite® 3880 Heat Cure Isotropic Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer Loctite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® 3880 Heat Cure Isotropic Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Electrically Conductive BondersLoctite® Electrically Conductive Adhesives are used in a variety of applications where electrical connectivity is needed, providing a conductive path where traditional methods such as solder, are not practical. Electrically Conductive Adhesives are ideal for attaching temperature sensitive components, or providing electrical interconnections on non-solderable substrates, such as plastic and glass.Loctite offers a complete line of electrically conductive adhesives to meet almost any need including: flexible, heat cure, room temperature cure, screen printable, high adhesion, and rapid cure.Loctite® 3880 Heat Cure Isotropic Epoxy AdhesiveA syringe or stencil dispense, heat cure, silver-conductive adhesive for solder replacement. Long work life. Can be stored in conventional refrigerator. Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 2.40 g/cc
0.0867 lb/in³
Mechanical Properties Metric English Comments
Adhesive Bond Strength >= 6.89 MPa
>= 1000 psi
Aluminum to Aluminum
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C

@Temperature 20.0 °C
25.0 µin/in-°F

@Temperature 68.0 °F
Glass Transition Temp, Tg 40.0 °C
104 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.00050 ohm-cm
<= 0.00050 ohm-cm
Processing Properties Metric English Comments
Cure Time 3.00 min
0.0500 hour
10 min. @ 125ºC, 6 min. @ 150ºC, 3 min. @ 175ºC
Pot Life 10080 min

@Temperature 23.0 °C
10080 min

@Temperature 73.4 °F
Shelf Life 6.00 Month
6.00 Month
1 component life at 0ºC