Polymer Property : Roll Temperature = 194 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® ABS 1410
PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® ABS 1415 Conductive Thermoplastic Compound
PRE-ELEC® ABS 1415 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® ABS..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® PA 1412 Conductive Thermoplastic Compound
PRE-ELEC® PA 1412 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® PC 1431
PRE-ELEC PC 1431 is a conductive thermoplastic compound based on polycarbonate. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® PC/ABS 1420
PRE-ELEC PC/ABS 1420 is a conductive thermoplastic compound based on a PC/ABS blend. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PR..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® PET 1451
PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® PP 1386
PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® PP 1391 Conductive Thermoplastic Compound
PRE-ELEC® PP 1391 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® PP 1393 Conductive Thermoplastic Compound
PRE-ELEC® PP 1393 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity,..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound
PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® PP 1396 Conductive Thermoplastic Compound
PRE-ELEC® PP 1396 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound
PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® PS 1324
PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® PS 1326
PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® PS 1331 Carbon Black Filled Conductive Thermoplastic Compound
PRE-ELEC® PS 1331 is a carbon black filled conductive thermoplastic compound based on polystyrene. In addition to a low electrical resistivity PRE-ELEC® PS 1331 has excellent mechanical properties..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® CP 1318  (discontinued **)
PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit..
Roll Temperature 90.0 °C
194 °F
1st Roll
Premix Thermoplastics PRE-ELEC® PPE 1461  (discontinued **)
PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric..
Roll Temperature 90.0 °C
194 °F
1st
Kostat E-2001 Conductive PP Compound
KOSTAT E-2001 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using a special conductive carbon black. In addition to a low electrical resistivity, E-200..
Roll Temperature 90.0 °C
194 °F
1st
Kostat E-3007J Conductive PS Compound
KOSTAT E-3007J is a conductive thermoplastic compound based on impact modified polystyrene and a special conductive carbon black.KOSTAT E-3007J is not dependant on atmospheric conditions.Special Fea..