Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 180 - 360 min | 3.00 - 6.00 hour | Anaerobic working strength |
Permabond UV7141 UV-curable Adhesive Permabond UV7141 is a UV-curable adhesive with a secondary anaerobic cure mechanism. This makes it ideal for bonding materials such as ceramic-coated glass, mirrors, etc. where UV-light cannot penet.. |
|||
Cure Time | 300 - 360 min | 5.00 - 6.00 hour | 5 to 6 hours to send at 77°F. |
Fibre Glast 1100 Light-Weight High-Strength Patching/Filler Compound Product Features:Very Light Weight MaterialNon-Hazardous Product - Safe to UseEasily Sanded and Carved with Shop ToolsNegligible ShrinkageNon-Critical, 2 to 1 Ratio by Weight or by VolumeExcellent N.. |
|||
Cure Time | 240 - 360 min @Temperature 23.0 °C |
4.00 - 6.00 hour @Temperature 73.4 °F |
|
Lord Adhesives Aeroglaze® M1433 Elastomeric Polyurethane Rain Erosion Coating Aeroglaze® M1433 elastomeric coating functions exceptionally well in abrasive environments. Inherent flexibility, corrosion resistance, and energy absorptive properties make Aeroglaze M1433 elast.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Dry Hard |
Lord Adhesives Chemglaze® M331 Elastomeric Polyurethane Chemglaze® M331 is a two package, ASTM D-16 Type IV elastomeric polyurethane coating. Cured films produced from this coating are tough, flexible, and resistant to erosion, abrasion, and impact. T.. |
|||
Cure Time | 240 - 360 min @Temperature 23.0 °C |
4.00 - 6.00 hour @Temperature 73.4 °F |
|
Master Bond EP39-2 Fast Curing Optically Clear Two Component Epoxy System Master Bond Polymer System EP39-2 is a fast curing, low viscosity, optically clear two component epoxy system for high performance bonding, sealing, coating and casting. It is 100% reactive and does.. |
|||
Cure Time | 240 - 360 min @Temperature 23.0 °C |
4.00 - 6.00 hour @Temperature 73.4 °F |
|
Master Bond EP51 Fast Curing High Bond Strength Epoxy Adhesive Master Bond Polymer Adhesive EP51 is a fast "5 minute" curing two component epoxy adhesive for general purpose bonding formulated to cure at room temperature with a one-to-one mix ratio by weight or.. |
|||
Cure Time | 240 - 360 min @Temperature 23.0 °C |
4.00 - 6.00 hour @Temperature 73.4 °F |
|
Master Bond EP51HT Fast Curing High Temperature Resistant Epoxy Adhesive Master Bond Polymer Adhesive EP51HT represents a significant advance in epoxy adhesive technology featuring an excellent balance of performance properties, including convenient curing at ambient tem.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | |
Trelleborg Emerson & Cuming Stycast® 4952/25 Two-Component Silicone High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Cure Time | 60.0 - 360 min | 1.00 - 6.00 hour | Full Cure; Primed |
Loctite® Gasket Eliminator® 509 Flange Sealant Anaerobic GasketingLoctite® 509 Flexible Cure Gasket Eliminator® Flange SealantProduct withstands minor flange movements caused by vibrations. It will not run when applied to vertical surfaces. F.. |
|||
Cure Time | 240 - 360 min @Temperature 121 °C |
4.00 - 6.00 hour @Temperature 250 °F |
|
Cotronics Duralco™ 4703 Adhesive and Tooling Compound High temperature resin reinforced with ceramic and metallic fibers and particles, resulting in high thermal stability. Easily machined to close tolerances and will repair and rebuild worn or cracke.. |
|||
Cure Time | 300 - 360 min | 5.00 - 6.00 hour | |
3M AC-770 Class B-1 Aerospace Sealant 3M Aerospace Sealant AC-770 Class B are fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealants. 3M AC-770 Class B Sealants have outstanding resistance to aviatio.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with QM CAT PURPLE |
ACC QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is us.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with QM CAT PURPLE |
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with QM CAT PURPLE |
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with QM CAT 135 |
ACC QM 135 QSI Quantum Silicones 35 Durometer Condensation Cured Moldmaking Material QM 135 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with QM CAT 140 |
ACC QM 140 QSI Quantum Silicones 40 Durometer Condensation Cured Moldmaking Material QM 140 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with Moldmaster Green |
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with Moldmaster Purple |
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with QM CAT PURPLE |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Cure Time | 300 - 360 min | 5.00 - 6.00 hour | Full Hardness |
3M Scotchkote™ 165CS Urethane Sealer Scotchkote Urethane Sealer 165CS has been specifically developed as a low viscosity primer/sealer for concrete and cementitious surfaces prior to application of other Scotchkote urethane systems.Pro.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with Moldmaster Green |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with Moldmaster Purple |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | demold time |
BCC Products BC 8690E Polyurethane Elastomer BC 8690E is a two-component urethane elastomer compound specifically designed for casting applications. This product is a safe, easy-to-handle, room temperature mixing and curing system that contain.. |
|||
Cure Time | 180 - 360 min | 3.00 - 6.00 hour | 2-4 hr at 200°F followed by 1-2 hr at 350°F |
Aremco Cerama-Dip™ 538-N High Temperature Specialty Ceramic-Inorganic Coating Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available. |
|||
Cure Time | 180 - 360 min | 3.00 - 6.00 hour | 2-4 hr at 200°F followed by 1-2 hr at 350°F |
Aremco Cerama-Dip™ 538-N-BLK High Temperature Specialty Ceramic-Inorganic Coating Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available. |
|||
Cure Time | 180 - 360 min | 3.00 - 6.00 hour | 2-4 hr at 200°F followed by 1-2 hr at 350°F |
Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with QM CAT PURPLE |
ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material QM 113 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Cure Time | 60.0 - 360 min | 1.00 - 6.00 hour | Full Cure; Primed |
Loctite® 573 Semi-rigid Cure Anaerobic Sealant Anaerobic GasketingLoctite® 573 Semi-rigid Cure Anaerobic SealantRecommended Primer: 7649 (N). Typical Use: Slow curing for extended assembly operations |