Polymer Property : Cure Time = 240 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 240 min
4.00 hour
On steel (fixture)
ND Industries 460 Instant High Pressure Pipe Sealant
High temperature, high strength general purpose stainless steel and other inert metals. For metal fittings
Cure Time 240 min
4.00 hour
Full cure
Resinlab® CYNERGY CA6302 Adhesive
Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl..
Cure Time 240 min
4.00 hour
Full cure
Resinlab® CYNERGY CA6309 Adhesive
Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl..
Cure Time 240 min
4.00 hour
Lord Adhesives 510 Fast Cure Acrylic Adhesive
Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi..
Cure Time 240 min
4.00 hour
Fixture time
ITW Devcon Safety Clear Coatâ„¢ Epoxy, Water Clear
Information provided by ITW Devcon
Cure Time 240 min

@Temperature 200 °C
4.00 hour

@Temperature 392 °F
Post Cure
Shin-Etsu Silicones KEG-2000-30A/B Elastomer
KEG-2000-30 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy..
Cure Time 240 min

@Temperature 200 °C
4.00 hour

@Temperature 392 °F
Post
Shin-Etsu Silicones KEG-2001-70A/B Fast Curing LIMS Silicone Rubber
ShinEtsu KEG200170 is a very fast cure liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. The viscosity of KEG20..
Cure Time 240 min

@Temperature 200 °C
4.00 hour

@Temperature 392 °F
Post
Shin-Etsu Silicones SF-11500U Fluorosilicone Elastomer
SF11500U is a low Durometer and low modulus fluorosilicone with excellent processing ability.. Typical Applications: GasketsSealsInformation Provided by Shin-Etsu Silicones of America, Inc.
Cure Time 240 min

@Temperature 200 °C
4.00 hour

@Temperature 392 °F
Post
Shin-Etsu Silicones SV-16000U Silicone Rubber
SV16000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Feat..
Cure Time 240 min

@Temperature 200 °C
4.00 hour

@Temperature 392 °F
Post
Shin-Etsu Silicones KE-5530U Low Temperature Silicone Elastomer
ShinEtsu KE5530 U is a nominal 30 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a..
Cure Time 240 min

@Temperature 205 °C
4.00 hour

@Temperature 401 °F
Post
Shin-Etsu Silicones KE-9611U Silicone Elastomer
KE9611 U is one of a series of easy processing, general purpose silicone rubber bases. It can be used in a variety of applications requiring finishing by molding (compression, injection, transfer).P..
Cure Time 240 - 480 min
4.00 - 8.00 hour
Tack-free
Sika Industry SikaFlex 201 Adhesive
Sika 201 SikaFlex AdhesiveSikaflex 201 meets Federal Specification TT-S-00230C, Type II, Class A and ASTK C-920, Type S, Grade NS. 15 - 15 mm Cut-Off. Good non-sag. Available in black, white, gray, ..
Cure Time 240 min

@Temperature 75.0 °C
4.00 hour

@Temperature 167 °F
Tra-Con Tra-Bond 927-1 Polysulfide Adhesive
TRA-BOND 927-1 thermally conductive polysulfide adhesive is designed for heat sink bonding applications. Information provided by Tra-Con Inc.
Cure Time 240 min
4.00 hour
2 hrs @ 75°C + 2 hrs @ 100°C
Tra-Con Tra-Bond 9070D Filled Epoxy Adhesive
TRA-BOND 9070D filled epoxy adhesive exhibits a low coefficient of expansion. Information provided by Tra-Con Inc.
Cure Time 240 min

@Temperature 121 °C
4.00 hour

@Temperature 250 °F
Cotronics 4700 Ultra Temp Adhesive and Casting Epoxy, General Purpose
Cure Time 240 min
4.00 hour
3M AC-240 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan..
Cure Time 240 min
4.00 hour
Tack-Free Time
3M AC-251 Black Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-251 Black Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate ai..
Cure Time 240 min
4.00 hour
Tack-Free Time
3M AC-251 Gray Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-251 Gray Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate air..
Cure Time 240 min
4.00 hour
3M AC-251 Gray Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-251 Gray Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate air..
Cure Time 240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with QM CAT 135
ACC QM 135 QSI Quantum Silicones 35 Durometer Condensation Cured Moldmaking Material
QM 135 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho..
Cure Time 240 min
4.00 hour
Time to Handling Strength
3M Scotch-Weld™ DP620NS Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesive DP-620NS is a back, long working time, two-component polyurethane. Formulated as 1:1 ratio liquids. With the squeeze of the trigger, or with automated dispensing..
Cure Time 240 min
4.00 hour
Time to Handling Strength
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Cure Time 240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with Moldmaster Purple
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material
QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch..
Cure Time 240 - 360 min
4.00 - 6.00 hour
Trelleborg Emerson & Cuming Stycast® 4640-25 Two-Component Silicone Flexible Encapsulant
Emerson & Cuming 4640-25 Stycast® Two-Component Silicone Flexible EncapsulantDescriptionAn RTV condensation cure. Pourable and room temperature curable.FeaturesHigh TemperaturePoor Chemical Resista..
Cure Time 240 - 1440 min
4.00 - 24.0 hour
Full Cure; Unprimed
Loctite® Gasket Eliminator® 510 Flange Sealant
Anaerobic GasketingLoctite® 510 High Temperature Rigid Cure Gasket Eliminator® Flange SealantProduct has a temperature range to 400ºF with excellent solvent and chemical resistance. Makes or dre..