Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ACC QM 140 QSI Quantum Silicones 40 Durometer Condensation Cured Moldmaking Material

Category Polymer , Thermoset , Silicone
Manufacturer Amber Chemical Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC QM 140 QSI Quantum Silicones 40 Durometer Condensation Cured Moldmaking Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QM 140 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent choice for the molding of intricate patterns, skin molding and applications where high durometer, dimensional stability and extremely tough rubber are required. Complies with FDA indirect food contact regulation CFR 177.2600 when used with Cat Clear FG. Refer to Cat Clear FG data sheet for specific properties.Key Features: Low viscosity High tear strength Fast demold time Excellent dimensional stabilityMain Applications: Molds for polyester, polyurethane and epoxy resin castings Molds for technical articles and prototype Molds for furniture and picture frame replication Part of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
Uncatalyzed, QM CAT 140
1.16 g/cc
1.16 g/cc
Base
1.31 g/cc
1.31 g/cc
catalyzed with QM CAT 140
Viscosity 250 cP
250 cP
Uncatalyzed, QM CAT 140
37000 cP
37000 cP
catalyzed with QM CAT 140
50000 cP
50000 cP
Base
Linear Mold Shrinkage <= 0.0030 cm/cm
<= 0.0030 in/in
cured 72 hrs @ RT
Storage Temperature <= 38.0 °C
<= 100 °F
6 months
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
cured 72 hrs @ RT
Tensile Strength, Yield 4.50 MPa
653 psi
cured 72 hrs @ RT
Elongation at Break 300 %
300 %
cured 72 hrs @ RT
Tear Strength 28.0 kN/m
160 pli
B, cured 72 hrs @ RT
Processing Properties Metric English Comments
Dry Time 12 - 16 hour
12 - 16 hour
Demold time, catalyzed with QM CAT 140
Cure Time 240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with QM CAT 140
Descriptive Properties Value Comments
Color Beige
Base
Light Purple
catalyzed with QM CAT 140
Purple
Uncatalyzed, QM CAT 140
Work Life 45 mins
catalyzed with QM CAT 140
Copyright © lookpolymers.com All Rights Reserved