Processing Properties Metric English Comments
Cure Time 180 - 360 min
3.00 - 6.00 hour
Anaerobic working strength
Permabond UV7141 UV-curable Adhesive
Permabond UV7141 is a UV-curable adhesive with a secondary anaerobic cure mechanism. This makes it ideal for bonding materials such as ceramic-coated glass, mirrors, etc. where UV-light cannot penet..
Cure Time 300 - 360 min
5.00 - 6.00 hour
5 to 6 hours to send at 77°F.
Fibre Glast 1100 Light-Weight High-Strength Patching/Filler Compound
Product Features:Very Light Weight MaterialNon-Hazardous Product - Safe to UseEasily Sanded and Carved with Shop ToolsNegligible ShrinkageNon-Critical, 2 to 1 Ratio by Weight or by VolumeExcellent N..
Cure Time 240 - 360 min

@Temperature 23.0 °C
4.00 - 6.00 hour

@Temperature 73.4 °F
Lord Adhesives Aeroglaze® M1433 Elastomeric Polyurethane Rain Erosion Coating
Aeroglaze® M1433 elastomeric coating functions exceptionally well in abrasive environments. Inherent flexibility, corrosion resistance, and energy absorptive properties make Aeroglaze M1433 elast..
Cure Time 240 - 360 min
4.00 - 6.00 hour
Dry Hard
Lord Adhesives Chemglaze® M331 Elastomeric Polyurethane
Chemglaze® M331 is a two package, ASTM D-16 Type IV elastomeric polyurethane coating. Cured films produced from this coating are tough, flexible, and resistant to erosion, abrasion, and impact. T..
Cure Time 240 - 360 min

@Temperature 23.0 °C
4.00 - 6.00 hour

@Temperature 73.4 °F
Master Bond EP39-2 Fast Curing Optically Clear Two Component Epoxy System
Master Bond Polymer System EP39-2 is a fast curing, low viscosity, optically clear two component epoxy system for high performance bonding, sealing, coating and casting. It is 100% reactive and does..
Cure Time 240 - 360 min

@Temperature 23.0 °C
4.00 - 6.00 hour

@Temperature 73.4 °F
Master Bond EP51 Fast Curing High Bond Strength Epoxy Adhesive
Master Bond Polymer Adhesive EP51 is a fast "5 minute" curing two component epoxy adhesive for general purpose bonding formulated to cure at room temperature with a one-to-one mix ratio by weight or..
Cure Time 240 - 360 min

@Temperature 23.0 °C
4.00 - 6.00 hour

@Temperature 73.4 °F
Master Bond EP51HT Fast Curing High Temperature Resistant Epoxy Adhesive
Master Bond Polymer Adhesive EP51HT represents a significant advance in epoxy adhesive technology featuring an excellent balance of performance properties, including convenient curing at ambient tem..
Cure Time 240 - 360 min
4.00 - 6.00 hour
Trelleborg Emerson & Cuming Stycast® 4952/25 Two-Component Silicone High Service Temp Encapsulant
Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har..
Cure Time 60.0 - 360 min
1.00 - 6.00 hour
Full Cure; Primed
Loctite® Gasket Eliminator® 509 Flange Sealant
Anaerobic GasketingLoctite® 509 Flexible Cure Gasket Eliminator® Flange SealantProduct withstands minor flange movements caused by vibrations. It will not run when applied to vertical surfaces. F..
Cure Time 240 - 360 min

@Temperature 121 °C
4.00 - 6.00 hour

@Temperature 250 °F
Cotronics Duralco™ 4703 Adhesive and Tooling Compound
High temperature resin reinforced with ceramic and metallic fibers and particles, resulting in high thermal stability. Easily machined to close tolerances and will repair and rebuild worn or cracke..
Cure Time 300 - 360 min
5.00 - 6.00 hour
3M AC-770 Class B-1 Aerospace Sealant
3M Aerospace Sealant AC-770 Class B are fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealants. 3M AC-770 Class B Sealants have outstanding resistance to aviatio..
Cure Time 240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with QM CAT PURPLE
ACC QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material
QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is us..
Cure Time 240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with QM CAT PURPLE
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material
QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an..
Cure Time 240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with QM CAT PURPLE
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material
QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili..
Cure Time 240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with QM CAT 135
ACC QM 135 QSI Quantum Silicones 35 Durometer Condensation Cured Moldmaking Material
QM 135 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho..
Cure Time 240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with QM CAT 140
ACC QM 140 QSI Quantum Silicones 40 Durometer Condensation Cured Moldmaking Material
QM 140 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho..
Cure Time 240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with Moldmaster Green
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material
QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch..
Cure Time 240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with Moldmaster Purple
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material
QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch..
Cure Time 240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with QM CAT PURPLE
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material
QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f..
Cure Time 300 - 360 min
5.00 - 6.00 hour
Full Hardness
3M Scotchkote™ 165CS Urethane Sealer
Scotchkote Urethane Sealer 165CS has been specifically developed as a low viscosity primer/sealer for concrete and cementitious surfaces prior to application of other Scotchkote urethane systems.Pro..
Cure Time 240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with Moldmaster Green
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material
QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch..
Cure Time 240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with Moldmaster Purple
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material
QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch..
Cure Time 240 - 360 min
4.00 - 6.00 hour
demold time
BCC Products BC 8690E Polyurethane Elastomer
BC 8690E is a two-component urethane elastomer compound specifically designed for casting applications. This product is a safe, easy-to-handle, room temperature mixing and curing system that contain..
Cure Time 180 - 360 min
3.00 - 6.00 hour
2-4 hr at 200°F followed by 1-2 hr at 350°F
Aremco Cerama-Dip™ 538-N High Temperature Specialty Ceramic-Inorganic Coating
Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.
Cure Time 180 - 360 min
3.00 - 6.00 hour
2-4 hr at 200°F followed by 1-2 hr at 350°F
Aremco Cerama-Dip™ 538-N-BLK High Temperature Specialty Ceramic-Inorganic Coating
Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.
Cure Time 180 - 360 min
3.00 - 6.00 hour
2-4 hr at 200°F followed by 1-2 hr at 350°F
Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating
Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.
Cure Time 240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with QM CAT PURPLE
ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material
QM 113 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an..
Cure Time 60.0 - 360 min
1.00 - 6.00 hour
Full Cure; Primed
Loctite® 573 Semi-rigid Cure Anaerobic Sealant
Anaerobic GasketingLoctite® 573 Semi-rigid Cure Anaerobic SealantRecommended Primer: 7649 (N). Typical Use: Slow curing for extended assembly operations
Copyright © lookpolymers.com All Rights Reserved