Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1013THL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1033THL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1040MHL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (Cond) Information provided by Ravago. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N2033HL Nylon 6 (DAM) Information provided by Ravago. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N2040MHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1013L Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1013STL Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1033L Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
Gromax PBT 3030-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | |
LTL Color Compounds ColorFast® NY2GF130 Nylon 66, 13% Glass-Filled 13% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-1373G Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-1674C Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-7010-45NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-7200-73 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Automotive Specifications: Chrysler MS-AK91; FORD WSS-M2D510-A7; .. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® 220-N Unfilled Nylon 66, Not Lubricated, Nucleated, or Heat Stabilized Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® 42LH-N Unfilled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® FRGF25-66-N Flame Retardant Nylon 66, Lubricated, 25% Glass Fiber Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® GF20-60 XE-N 20% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® GF33-66/6 XE-N 33% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® GS40-60 42LH-N 40% Glass Sphere Filled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® MR409 22H-N 40% Mineral Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® MR410 42H-N 40% Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® XT1486-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-1141A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-2420H Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | |
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S.. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
Gromax CCP PBT 6730-104F Glass/Mineral Filled Product Description: PBT glass/mineral reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent w.. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | |
LTL Color Compounds ColorFast® NY1GF330 Nylon 6, 33% Glass-Filled 33% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |