Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
RheTech Products FRP300-01 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
NatureWorks® Ingeo™ 3251D Injection Grade PLA IngeoTM Biopolymer 3251D is designed for injection molding applications. This polymer grade has a higher melt flow capability than other IngeoTM resins currently in the market place. The higher flow.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
ExxonMobil Vyram™ 9101-65 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
NOVA Chemicals Dylark® 378P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 100 psi | |
Fiberfil® J-60/20/E Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 100 psi | |
Fiberfil® J-60/30/FR Polypropylene Homopolymer, 30% Glass Fiber Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 100 psi | |
Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Injection Molding |
Ineos ABS Lustran® 288 ABS, Injection Molding Grade Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Star Plastics ABS9020 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass Information provided by Star Plastics, Inc. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP 1097 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP 1227D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-1277B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-1451L Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-1709C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-2024A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-2249 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-2760BR Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-2850E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-1878 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer
(discontinued **) A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
ExxonMobil Santoprene® 211-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
ExxonMobil Santoprene® 211-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
LTL Color Compounds ColorFast® NY1GF130 Nylon 6, 13% Glass-Filled 13% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
ExxonMobil Santoprene® 101-73 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |