Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex MONPRENE® MP 2850E Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Teknor Apex Company
Trade Name MONPRENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex MONPRENE® MP 2850E Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Melt Flow 1.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 53
53
ASTM D2240
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Elongation at Break 700 %
700 %
ASTM D412
300% Modulus 0.00207 GPa
0.300 ksi
ASTM D412
Compression Set 20 %
20 %
23°C, 22 hr.; ASTM D395, Method B
60 %
60 %
70°C, 22 hr.; ASTM D395, Method B
Users viewing this material also viewed the following: