Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.200 - 0.500 MPa | 29.0 - 72.5 psi | |
Polykemi AB POLYelast TPE EC12 D55 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Back Pressure | 0.200 - 0.500 MPa | 29.0 - 72.5 psi | |
Polykemi AB POLYelast TPE EC88R Thermoplastic Elastomer, PP/EPDM Information provided by Polykemi AB |
|||
Back Pressure | 0.200 - 0.500 MPa | 29.0 - 72.5 psi | |
Polykemi AB POLYelast TPE R44 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Back Pressure | 0.200 - 0.500 MPa | 29.0 - 72.5 psi | |
Polykemi AB POLYelast TPE R44 TV10 Thermoplastic Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Back Pressure | 0.200 - 0.500 MPa | 29.0 - 72.5 psi | |
Polykemi AB POLYelast TPE ZC100 D40 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Back Pressure | 0.200 - 0.500 MPa | 29.0 - 72.5 psi | |
Polykemi AB POLYelast TPE R44 T10 Thermoplastic Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Back Pressure | 0.200 - 0.650 MPa | 29.0 - 94.3 psi | |
Akro-Plastic Akromid® T1 GF 30 (3466) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Back Pressure | 0.200 - 0.650 MPa | 29.0 - 94.3 psi | |
Akro-Plastic Akromid® T1 GF 30 9 (3498) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Back Pressure | 0.200 - 0.650 MPa | 29.0 - 94.3 psi | |
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Back Pressure | 0.200 - 0.650 MPa | 29.0 - 94.3 psi | |
Akro-Plastic Akromid® T1 GF 50 9 (3257) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Back Pressure | 0.200 - 0.650 MPa | 29.0 - 94.3 psi | |
Akro-Plastic Akromid® T6 GF 50 (3106) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Back Pressure | 0.200 - 0.650 MPa | 29.0 - 94.3 psi | |
Akro-Plastic Akromid® T6 GF30 (3501) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Back Pressure | 0.200 - 1.00 MPa | 29.0 - 145 psi | |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Conditioned (2.5% Moisture) Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Back Pressure | 0.200 - 1.00 MPa | 29.0 - 145 psi | |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Back Pressure | 0.200 - 0.650 MPa | 29.0 - 94.3 psi | |
Akro-Plastic Akromid® T1 GF 40 (3464) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Back Pressure | 0.200 - 0.650 MPa | 29.0 - 94.3 psi | |
Akro-Plastic Akromid® T1 GF 40 9 (3499) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Back Pressure | 0.200 - 0.650 MPa | 29.0 - 94.3 psi | |
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Back Pressure | 0.200 - 1.00 MPa | 29.0 - 145 psi | |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
Back Pressure | 0.200 - 1.00 MPa | 29.0 - 145 psi | |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Back Pressure | 0.200 - 1.00 MPa | 29.0 - 145 psi | |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |