Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 2 - 8 hour | 2 - 8 hour | in fresh-air dryer |
Polykemi AB POLYblend 45FS GKF2010 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in fresh-air dryer |
Polykemi AB POLYblend 45FS PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in fresh-air dryer |
Polykemi AB POLYblend 45V GF10 PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in desiccant air dryer |
Polykemi AB POLYblend 45V GF10 PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in circulation dryer |
Polykemi AB POLYblend 65 M10 PC/ABS-blend, Reinforced Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in fresh-air dryer |
Polykemi AB POLYblend 65CI PC/ABS-Blend Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in desiccant air dryer |
Polykemi AB POLYblend 65CI PC/ABS-Blend Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in circulation dryer |
Polykemi AB POLYblend 65FS LB PC/ABS-Blend Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in fresh-air dryer |
Polykemi AB POLYblend 65FS PC/ABS-Blend Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in desiccant air dryer |
Polykemi AB POLYblend 85FS UV PC/ABS-Blend, UV stabilized Information provided by Polykemi AB |
|||
Dry Time | 2 - 8 hour | 2 - 8 hour | in circulation dryer |
Polykemi AB POLYblend C65HF PC/ABS-blend Information provided by Polykemi AB |
|||
Dry Time | 4 - 8 hour | 4 - 8 hour | |
Lanxess Pocan® DP 7102 000000 PBT, 32% Mineral PBT, 32% mineral, injection molding, LDSInformation provided by LANXESS. |
|||
Dry Time | 4 - 8 hour | 4 - 8 hour | |
Lanxess Pocan® ECO T 3220 000000 PBT + PET, 20% Glass Fiber PBT + PET, 20% glass fibers, injection molding, improved surface finish, contains 28% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | |
MRC Polymers NAXALOYâ„¢ 793A3 GF10 PC and Polyester Blend, 10% Glass Fiber Filled 793 GF10 is available in natural and custom colors, internal and external lubricants, UV stabilizer and other modifications.Information provided by MRC Polymers Inc. |
|||
Dry Time | 4 - 8 hour | 4 - 8 hour | |
Lanxess Pocan® C 1202 000000 PET + PC PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3020X15 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3024U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030JLX1 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability (DIN 73378 Nomenclature = PA12 PHL)Information provided by UBE. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Hydrochloric Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Oil (ASTM D471 No. 1) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Saturate Sodium Chloride for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Isopropanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Methanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Saturate Sodium Chloride for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030XA Nylon 12 Film Description: UBESTA Nylon 12 FilmInformation provided by UBE. |
|||
Dry Time | 4 - 8 hour | 4 - 8 hour | |
Akro-Plastic Akroloy® PA GF 30 (2718) PA 6.6 & PA6I/6T Dry, 30% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Dry Time | 4 - 8 hour | 4 - 8 hour | |
Beijing Chemical Industry KAIFA® 2030 PET Resin High mechanical strength, Creep resistant, Low frictionInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® 3030LUX 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: rigid, stabilized against weatherability (DIN 73378 Nomenclature = PA12 HL)Information provided by UBE. |
|||
Dry Time | 6 - 8 hour | 6 - 8 hour | Option 1 |
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |