Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 149 - 163 °C | 300 - 325 °F | Average value: 149 °C Grade Count:13 |
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an.. |
|||
Drying Temperature | 149 - 163 °C | 300 - 325 °F | |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU)
(Unverified Data**) Udel GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resista.. |
|||
Drying Temperature | 149 - 163 °C | 300 - 325 °F | |
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU)
(Unverified Data**) Udel GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi.. |
|||
Drying Temperature | 135 - 163 °C | 275 - 325 °F | |
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)
(Unverified Data**) Udel P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand prolonged e.. |
|||
Drying Temperature | 135 - 163 °C | 275 - 325 °F | |
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)
(Unverified Data**) Udel P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and withsta.. |
|||
Drying Temperature | 135 - 163 °C | 275 - 325 °F | |
Solvay Specialty Polymers Udel® P-1720 Polysulfone (PSU)
(discontinued **) Udel P-1720 is a flame-retardant grade of polysulfone (PSU) that has a UL94 rating of V-0 at a thickness of 1 mm (0.039"). In general, polysulfone is a tough, rigid, high-strength thermoplastic that.. |
|||
Drying Temperature | 135 - 163 °C | 275 - 325 °F | |
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU)
(Unverified Data**) Udel P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded. Polysulfones have long been known for trans.. |
|||
Drying Temperature | 135 - 163 °C | 275 - 325 °F | |
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)
(Unverified Data**) Udel P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion. Th.. |
|||
Drying Temperature | 135 - 163 °C | 275 - 325 °F | |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)
(Unverified Data**) Udel polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel P-3500 LCD MB series polymers are particularly well suited for the fabrication of porous .. |
|||
Drying Temperature | 135 - 163 °C | 275 - 325 °F | |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU)
(Unverified Data**) Udel P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel P-1700 and a slightly greater t.. |
|||
Drying Temperature | 135 - 163 °C @Time 10800 - 14400 sec |
275 - 325 °F @Time 3.00 - 4.00 hour |
|
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat.. |
|||
Drying Temperature | 135 - 163 °C @Time 10800 - 14400 sec |
275 - 325 °F @Time 3.00 - 4.00 hour |
|
Solvay Specialty Polymers Mindel® B-430 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-430 is a 30% glass reinforced thermoplastic with excellent dimensional stability, exceptional resistance to warp, good chemical resistance, and high stiffness. It was developed specifically.. |
|||
Drying Temperature | 135 - 163 °C | 275 - 325 °F | |
Solvay Specialty Polymers Udel® P-1800 Polysulfone (PSU)
(discontinued **) Udel P-1800 is a powdered grade of polysulfone with molecular weight similar to that of Udel P-1700 polysulfone. It is well suited for the fabrication of porous membranes that can be made into hollo.. |
|||
Drying Temperature | 149 - 163 °C | 300 - 325 °F | |
PolyOne Edgetek® LCP-15GF/000 Liquid Crystal Polymer - 15% Fiber Glass
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 149 - 163 °C | 300 - 325 °F | |
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 149 - 163 °C @Time 10800 - 14400 sec |
300 - 325 °F @Time 3.00 - 4.00 hour |
|
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU), Glass Fiber Udel® GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical res.. |
|||
Drying Temperature | 149 - 163 °C @Time 10800 - 14400 sec |
300 - 325 °F @Time 3.00 - 4.00 hour |
|
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU), Glass Fiber Udel® GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical .. |
|||
Drying Temperature | 135 - 163 °C @Time 12600 sec |
275 - 325 °F @Time 3.50 hour |
|
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU) Udel® P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and.. |
|||
Drying Temperature | 135 - 163 °C @Time 12600 sec |
275 - 325 °F @Time 3.50 hour |
|
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU) Udel® P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded.Polysulfones have long been known for tr.. |
|||
Drying Temperature | 135 - 163 °C @Time 12600 sec |
275 - 325 °F @Time 3.50 hour |
|
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU) Udel® polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel® P-3500 LCD MB series polymers are particularly well suited for the fabrication of.. |
|||
Drying Temperature | 135 - 163 °C @Time 12600 sec |
275 - 325 °F @Time 3.50 hour |
|
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU) Udel® P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion.. |
|||
Drying Temperature | 135 - 163 °C @Time 12600 sec |
275 - 325 °F @Time 3.50 hour |
|
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU) Udel® P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel® P-1700 and a slightly g.. |
|||
Drying Temperature | 135 - 163 °C @Time 12600 sec |
275 - 325 °F @Time 3.50 hour |
|
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU) Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand pro.. |