Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Pre-drying in a dehumidifier |
Premix Thermoplastics PRE-ELEC® ESD 5300 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5300 is a static dissipative thermoplastic compound based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance valu.. |
|||
Drying Temperature | 60.0 °C | 140 °F | |
Pasargad Polymer Peyvand Pasadur 3P-H8130B PBT, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Drying Temperature | 60.0 - 70.0 °C | 140 - 158 °F | Temperature can be reduced when using vacuum ovens. |
LATI LASTIROL TR-V0 Polystyrene (PS) (UL94 V-0)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Drying Temperature | 60.0 - 71.1 °C | 140 - 160 °F | |
PolyOne Edgetek® AS-20CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 60.0 - 70.0 °C | 140 - 158 °F | |
LG Chemical HI855HS PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Drying Temperature | 60.0 - 80.0 °C | 140 - 176 °F | ( 2 hrs) Pre drying temp. |
Supreme Petrochem SP 6411 1924 Light Stabilized Polystyrene Characteristics Prevents dust patterns due to static charges High gloss Good flow Improved light fastness Processing Injection molding Extrusion Applications A/C and cooler grill Material Status.. |
|||
Drying Temperature | 60.0 - 70.0 °C | 140 - 158 °F | Temperature can be reduced when using vacuum ovens. |
LATI LASTIROL TR G/10-V1 ES 10% Glass Fiber Polystyrene (PS) Structural Foam Resin (UL94 V-1)
(discontinued * Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Drying Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Injection Molding |
LG Chemical KEYFLEX TO1088AV Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0Information provided by LG Chemical |
|||
Drying Temperature | 60.0 - 70.0 °C | 140 - 158 °F | |
Arkema Group Pebax® MX 1205 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MX 1205 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information prov.. |