Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources AC-GP2-TFE5 Acetal Copolymer, 5% PTFE Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources PC/ABS-FRG5 Flame Retardant PC/ABS Alloy, 5% Glass Reinforced PC/ABS Alloy, Flame Retardant, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources PC/ABS-FR1-[color]-HH Flame Retardant PC/ABS Alloy, Low Flow PC/ABS Alloy, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources PC/ABS-GP1-[color]-LG General Purpose PC/ABS Alloy, Low Gloss Grade PC/ABS Alloy, General Purpose, Low Gloss GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
Drying Temperature | 76.7 °C | 170 °F | |
PolyOne Edgetek® AS-10CF/000 FR Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued Description/Features:Carbon Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-60/10 Polypropylene Homopolymer, 10% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-60/10/CC/30/E NATL Polypropylene Homopolymer, 10% FiberGlass and 30% Calcium Carbonate Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-60/10/E/M Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-60/30/E/HF Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, improved flow Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-60/40 Polypropylene Homopolymer, 40% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-60/40/E Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® M-1812 Polypropylene Homopolymer, 45% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® PP-60/CC/40 Polypropylene Homopolymer, 40% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® PP-62/MI/25 Polypropylene Copolymer, 25% Mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-60/15/MI/20 Polypropylene Homopolymer, 35% Glass/mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-60/20/E/HF Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled, improved flow Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-61/30/FR Polypropylene Copolymer, 30% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® PP-15/T/10/20 Polypropylene Homopolymer, 22% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 - 87.8 °C | 170 - 190 °F | |
MRC Polymers SATRANâ„¢ 800R ABS Terpolymer, Reprocessed black onlyInformation provided by MRC Polymers Inc. |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-68/20/E Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |