Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 149 - 188 °C | 300 - 370 °F | |
PolyOne Versaflex™ 9545-1 Thermoplastic Elastomer (TPE) Versaflex™ 9545-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Rear Barrel Temperature | 149 - 188 °C | 300 - 370 °F | |
PolyOne Versaflex™ 9555-1 Thermoplastic Elastomer (TPE) Versaflex™ 9555-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Rear Barrel Temperature | 149 - 188 °C | 300 - 370 °F | |
PolyOne Versaflex™ 9555-9 Thermoplastic Elastomer (TPE) Versaflex™ 9555-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Rear Barrel Temperature | 149 - 188 °C | 300 - 370 °F | |
PolyOne Versaflex™ 9570-9 Thermoplastic Elastomer (TPE) Versaflex™ 9570-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Rear Barrel Temperature | 171 - 188 °C | 340 - 370 °F | |
PolyOne Versaflex™ CL2242 Thermoplastic Elastomer (TPE) Versaflex™ CL2242 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Rear Barrel Temperature | 171 - 188 °C | 340 - 370 °F | |
PolyOne Versaflex™ CL2250 Thermoplastic Elastomer (TPE) Versaflex™ CL2250 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Rear Barrel Temperature | 166 - 188 °C | 331 - 370 °F | |
PolyOne Versaflex™ OM 1040X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1040X-1 is a medical compliant overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, A.. |
|||
Rear Barrel Temperature | 166 - 188 °C | 331 - 370 °F | |
PolyOne Versaflex™ OM 2262 Thermoplastic Elastomer (TPE) Versaflex™ OM 2262 is a performance overmolding grade with general FDA compliance. This product is designed for both insert and two-shot molding onto Eastman Tritan™ copolyester as well as ABS, PC.. |
|||
Rear Barrel Temperature | 149 - 188 °C | 300 - 370 °F | |
PolyOne Versalloy™ HC 9210-45N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-45N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgic.. |
|||
Rear Barrel Temperature | 149 - 188 °C | 300 - 370 °F | |
PolyOne Versalloy™ HC 9210-55N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-55N is a TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgical grips. Prod.. |
|||
Rear Barrel Temperature | 149 - 188 °C | 300 - 370 °F | |
PolyOne Versalloy™ XL 9070X-9 Thermoplastic Elastomer (TPE) Versalloy™ XL 9070X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Exceptional Flow for Long, Thin Flow Paths - Overmold Adhesion to Polyp.. |
|||
Rear Barrel Temperature | 163 - 188 °C | 325 - 370 °F | |
PolyOne Versollan™ OM 1262NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-1 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Excellent Grip with Matte, Rubbery Finish - Proven Track R.. |
|||
Rear Barrel Temperature | 163 - 188 °C | 325 - 370 °F | |
PolyOne Versollan™ RU 2204X Thermoplastic Elastomer (TPE) Versollan™ RU 2204X is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performan.. |
|||
Rear Barrel Temperature | 168 - 188 °C | 334 - 370 °F | |
PolyOne Versollan™ RU 2205-9 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-9 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Rear Barrel Temperature | 171 - 188 °C | 340 - 370 °F | |
PolyOne Dynaflex™ G7431-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7431-1001-00 is an easy processing, performance TPE designed for use in applications requiring a tough, durable material with a low coefficient of friction. - Excellent Heat Stability - .. |
|||
Rear Barrel Temperature | 160 - 188 °C | 320 - 370 °F | |
PolyOne Dynaflex™ G7630-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7630-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe.. |
|||
Rear Barrel Temperature | 160 - 188 °C | 320 - 370 °F | |
PolyOne Dynaflex™ G7630-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7630-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. *Made with Kraton® Polymer - Non.. |
|||
Rear Barrel Temperature | 160 - 188 °C | 320 - 370 °F | |
PolyOne Dynaflex™ G7650-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Rear Barrel Temperature | 166 - 188 °C | 331 - 370 °F | |
PolyOne Dynaflex™ G7680-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Rear Barrel Temperature | 149 - 188 °C | 300 - 370 °F | |
PolyOne Dynaflex™ G7680-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Rear Barrel Temperature | 160 - 188 °C | 320 - 370 °F | |
PolyOne Dynaflex™ G7940-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Rear Barrel Temperature | 166 - 188 °C | 331 - 370 °F | |
PolyOne Dynaflex™ G7980-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7980-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Rear Barrel Temperature | 166 - 188 °C | 331 - 370 °F | |
PolyOne Dynaflex™ G7990-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7990-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-9001-02 can be re.. |
|||
Rear Barrel Temperature | 177 - 188 °C | 350 - 370 °F | |
Polymer Resources AC-G10 Acetal Copolymer, 10% Glass Reinforced Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 149 - 188 °C | 300 - 370 °F | |
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O.. |
|||
Rear Barrel Temperature | 166 - 188 °C | 331 - 370 °F | |
PolyOne Dynaflex™ G7980-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7980-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Rear Barrel Temperature | 160 - 188 °C | 320 - 370 °F | |
PolyOne Dynalloy™ OBC 8100-N50 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N50 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Rear Barrel Temperature | 160 - 188 °C | 320 - 370 °F | |
PolyOne Dynalloy™ OBC 8100-N65 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N65 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Rear Barrel Temperature | 166 - 188 °C | 331 - 370 °F | |
PolyOne Dynalloy™ OBC8000-T60 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T60 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl.. |
|||
Rear Barrel Temperature | 166 - 188 °C | 331 - 370 °F | |
PolyOne Dynalloy™ OBC8200-BT50 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8200-BT50 is a translucent grade to be used in blow molding applications. New Product. Commercial specifications have not been established. - Excellent Colorability - Rubbery FeelPurge.. |