Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 120 - 140 °C | 248 - 284 °F | DAM |
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is also a PPA resin.Information provided by DuPont Performan.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA)
(Unverified Data**) Ixef GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without signi.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | Needed to develop high crystallinity |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Mold Temperature | 120 - 130 °C | 248 - 266 °F | |
LATI LASULF Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-7744 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-7950 Polyamide 46, with aramid reinforcement and PTFE, toughness-modified, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-8094 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-8250 Polyamide 46, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Highly dimensionally stable at elevated tem.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-8263 Polyamide 46, with carbon fiber and glass fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-8365 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Mold Temperature | 120 - 200 °C | 248 - 392 °F | |
Lehmann & Voss LUVOCOM® 1100-7939/GY Polyether sulfone, unreinforced Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feature.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® 2030 Polyarylamide (PARA), 55% GlassMineral Ixef® 2030 is a 55% glass-fiber/mineral reinforced polyarylamide compound which exhibits high strength, very high stiffness, low warpage, excellent creep resistance and outstanding surface gloss... |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® HC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® HC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | actual surface temp |
Unitika P-1001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Mold Temperature | 120 - 160 °C | 248 - 320 °F | |
Topas Advanced Polymers TOPAS® 6017S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6017S-04 is an injection molding grade with a high heat distortion temperature (170°C) and exceptional dimensional stability. It is a glass-clear amorphous polymer with outstanding moisture.. |
|||
Mold Temperature | 120 °C | 248 °F | |
Toyobo ECOVYLOPET® EMC2301E PET Bottle Recycling Grade, 15% Filler Reinforced Features: PET Bottle Recycling Grade, 15% Filler Reinforced, Modified TypeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Toyobo GLAMIDE® T-663G50A MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | actual surface temp |
Unitika P-1001A Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Eurotec® Tecopet® PT70 GR30 NL100 XD70 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), long-term heat stabilized, natural Information provided by Eurotec® |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Eurotec® Tecopet® PT74 GR20 BK002 XA20 PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black Information provided by Eurotec® |
|||
Mold Temperature | 120 - 125 °C | 248 - 257 °F | |
BecauseWeCare BF90 Biodegradable Plastic Biodegradable and compostable product produced from corn and developed to break down within weeks in a compost environment, without leaving any harmful residues in the process. Certified to the vari.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | Needed to develop high crystallinity |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM
(discontinued **)< The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | Needed to develop high crystallinity |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Mold Temperature | 120 - 160 °C | 248 - 320 °F | |
BASF Ultrason S 6010 PSU Ultrason S 6010 is an unreinforced, high molecular weight injection-molding and extrusion grade with excellent chemical resistance (stress crack resistance) and good solubility in typical solvents (.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | Needed to develop high crystallinity |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM
(discontinued **)&l Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® 5002 Polyarylamide (PARA), 20% GlassPTFE
(discontinued **) Ixef 5002 is a 20% glass-fiber reinforced, PTFE modified polyarylamide which exhibits very good mechanical performance, very good surface gloss, and superior wear properties.- Natural: Ixef 5002/008.. |