Processing Properties Metric English Comments
Mold Temperature 107 - 163 °C
225 - 325 °F
Oxford Polymers PPS/66-505-40GF-BK PPS/PA66, 40% Glass Fiber Reinforced
Product Description: Glass Fiber (40% Reinforced), Polyphenylene sulfide injection molding grade based alloy with Nylon 66 Processing and Delivery Form: Pellets and Injection MoldingAppearance: Bla..
Mold Temperature 107 - 177 °C
225 - 350 °F
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced
Polyetherimide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Mold Temperature 107 - 177 °C
225 - 350 °F
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced
Polyetherimide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Mold Temperature 107 - 177 °C
225 - 350 °F
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced
Polyetherimide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Mold Temperature 107 - 177 °C
225 - 350 °F
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced
Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Mold Temperature 107 - 177 °C
225 - 350 °F
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant
Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Mold Temperature 107 - 177 °C
225 - 350 °F
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant
Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Mold Temperature 107 - 180 °C
225 - 356 °F
Average value: 154 °C Grade Count:13
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea..
Mold Temperature 107 - 177 °C
225 - 350 °F
Average value: 152 °C Grade Count:4
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E..
Mold Temperature 107 - 177 °C
225 - 350 °F
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Mold Temperature 107 - 177 °C
225 - 350 °F
Polymer Resources PEI-GP1 Polyetherimide, General Purpose, Unreinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Mold Temperature 107 - 163 °C
225 - 325 °F
Solvay Specialty Polymers Radel® R-7120 Polyphenylsulfone, 20% glass fiber  (discontinued **)
RADEL R 7120 is a 20% glass fiber reinforced grade of RADEL R polyphenylsulfone developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 ..
Mold Temperature 107 - 163 °C
225 - 325 °F
Solvay Specialty Polymers Radel® R-7159 Polyphenylsulfone (PPSU)
Radel® R-7159 polyphenylsulfone (PPSU) was developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical burn..
Mold Temperature 107 - 163 °C
225 - 325 °F
Solvay Specialty Polymers Radel® R-7400 Polyphenylsulfone (PPSU)
Radel® R-7300 (for light colors) and R-7400 (for darker colors) polyphenylsulfone resins were developed specifically for aircraft interior applications, and through the use of a proprietary flame..
Mold Temperature 107 - 163 °C
225 - 325 °F
Solvay Specialty Polymers Radel® R-7535 Polyphenylsulfone (PPSU)
Radel® R-7535 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu..
Mold Temperature 107 - 163 °C
225 - 325 °F
Solvay Specialty Polymers Radel® R-7558 Polyphenylsulfone (PPSU)
Radel® R-7558 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu..
Mold Temperature 107 - 163 °C
225 - 325 °F
Solvay Specialty Polymers Radel® R-7625 Polyphenylsulfone (PPSU)
Radel® R-7625 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications that offers improved UV resistance versus Radel® R-7535 and Radel® R-7558. The product ..
Mold Temperature 107 - 121 °C
225 - 250 °F
PolyOne Lubri-Tech™ MP-000/10T Modified PPO - 10% PTFE  (discontinued **)
Data provided by PolyOne.
Mold Temperature 107 - 163 °C
225 - 325 °F
Solvay Specialty Polymers Radel® R-7300 Polyphenylsulfone (PPSU)
Radel® R-7300 (for light colors) and R-7400 (for darker colors) polyphenylsulfone resins were developed specifically for aircraft interior applications, and through the use of a proprietary flame r..
Mold Temperature 107 - 177 °C
225 - 350 °F
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Mold Temperature 107 - 177 °C
225 - 350 °F
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Mold Temperature 107 - 177 °C
225 - 350 °F
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Copyright © lookpolymers.com All Rights Reserved