Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Average value: 74.3 °C Grade Count:32 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® 6134 NC010 PBT
(Unverified Data**) Crastin® 6134 NC010 is an unreinforced, medium viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® HR5315HF BK503 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT
(Unverified Data**) Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® LW9320 BK851 PBT
(Unverified Data**) Crastin® LW9320 BK851 is a 20% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® LW9320LM BK591 PBT
(Unverified Data**) Crastin® LW9320LM is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. It has excellent surface aspect, dimensional stability and low warpage and was developed fo.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® S600F10 BK851 PBT
(Unverified Data**) Crastin® S600F10 BK851 is an unreinforced, lubricated, medium high viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® SK609 BK851 PBT
(Unverified Data**) Crastin® SK609 BK851 is a 50% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Injection Molding |
DuPont Performance Polymers Crastin® SK615SF BK591 PBT
(Unverified Data**) Crastin® SK615SF BK591 is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast .. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Injection Molding |
DuPont Performance Polymers Crastin® SK615SF NC010 PBT
(Unverified Data**) Crastin® SK615SF is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® SK645FR BK851 PBT
(Unverified Data**) Crastin® SK645FR BK851 is a flame retardant , 30% glass reinforced black polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.75mm.Information provided by DuPont Performance P.. |
|||
Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | Start Point: 90°C |
Kingfa JH720 G10D 10% Glass Fiber Reinforced PC Features:Good processing propertiesLow tendency to warpHigh mechanical strengthGood size stabilityGood surfaceSuitable for exact moldingApplications:Exact mechanism partsPrinter, photocopies, scanne.. |
|||
Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | Injection Molding |
LG Chemical LUCON SP9306FL sPS+MF Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 .. |
|||
Mold Temperature | 100 - 130 °C | 212 - 266 °F | |
Lanxess Pocan® DP T 7140 LDS 000000 PET + PBT, 42% Glass Fiber/Mineral PET + PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | Start Point: 100°C |
Kingfa JH710 G30 Flame Retardant & 30% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Mold Temperature | 120 - 130 °C | 248 - 266 °F | |
LATI Latiohm 80-05 CNT GCE/500 PPS, Glass/Mineral Reinforced Semiconductive/dissipative product based on Polyphenylene Sulfide (PPS). Carbon nanotubes. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Mold Temperature | 100 - 130 °C | 212 - 266 °F | |
LATI Latishield 85-08A G/20 PES, Steel/Glass Fibers EMI shielding product based on Polyether Sulfone (PES). Steel fibers. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
Solvay Specialty Polymers Kalix® 3850 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 3850 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in.. |
|||
Mold Temperature | 110 - 130 °C | 230 - 266 °F | |
Covestro Apec® 1795 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=173°CPreprocessingMax. Water content |
|||
Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
Covestro Makrolon® 9417 Polycarbonate, 10% Glass Filled ISO 7391-PC,MFLR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityUV stab.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® CE2056 NC010 PBT Crastin® CE2056 NC010 is an unreinforced polybutylene terephthalate molding resin.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® S600LF NC010 PBT Crastin® S600LF NC010 is an unreinforced, Teflon® PTFE powder lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Injection Molding |
DuPont Performance Polymers Crastin® SK612SF BK591 PBT Crastin® SK612SF BK591 is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast .. |
|||
Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
Covestro Makrolon® DP1-1887* Polycarbonate, 10% Glass Filled ISO 7391-PC,MR,(,,)-18-9,GF10Developmental productMVR (300 °C/1.2 kg) 16 cm3/10 min10 % Glass fiber reinforcedMilled fiberLow viscosityEasy releasegood surface qualityInjection molding - Melt tempe.. |
|||
Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
Covestro Makrolon® DP1-1888* Polycarbonate, 20% Glass Filled ISO 7391-PC,MR,(,,)-09-3,GF20Developmental productMVR (300 °C/1.2 kg) 10 cm3/10 min20 % Glass fiber reinforcedMilled fiberMedium viscosityEasy releasegood surface qualityInjection molding - Melt te.. |
|||
Mold Temperature | 100 - 130 °C | 212 - 266 °F | |
Akro-Plastic Akromid® T1 GF 30 9 (3498) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Mold Temperature | 110 - 130 °C | 230 - 266 °F | actual surface temp |
Unitika P-3001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Mold Temperature | 120 - 130 °C | 248 - 266 °F | |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® CE2055 BK580 PBT
(Unverified Data**) Crastin® CE2055 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Injection Molding |
DuPont Performance Polymers Crastin® S610SF NC010 PBT
(Unverified Data**) Crastin® S610SF is an unreinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast production.Informati.. |