Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 100 - 120 °C | 212 - 248 °F | |
NHEP Spectron™ E6666 Nylon 66, 30% Glass Fiber Natural color. E6666 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informati.. |
|||
Mold Temperature | 100 °C | 212 °F | optimum |
DuPont Performance Polymers Sorona® FG3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data** Sorona® FG3015G NC010 is a 15% glass fiber reinforced polytrimethylene terephthalate resin containing 31% renewably sourced ingredients by weight (37% based on polymer only) formulated to be food c.. |
|||
Mold Temperature | 100 - 150 °C | 212 - 302 °F | |
LATI LAESTRA G/30 30% Glass Fiber Reinforced Syndiotactic Polystyrene (SPS)
(discontinued **) Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |
|||
Mold Temperature | 100 °C | 212 °F | Injection Molding |
Covestro Apec® 1700 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay.. |
|||
Mold Temperature | 100 °C | 212 °F | Injection Molding |
Covestro Apec® DP 1-9339/5 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Mold Temperature | 100 - 120 °C | 212 - 248 °F | |
LATI LATILUB 95-25GR CE/10 Polysulfone Base (PSU), 25% Graphite, 10% Special Mineral Filled Self Lubricating Plastic Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Mold Temperature | 100 °C | 212 °F | DAM; optimum |
DuPont Performance Polymers Minlon® 10B140 BK061 Nylon 66
(Unverified Data**) Minlon® 10B140 BK061 is a 40% mineral reinforced, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 100 °C | 212 °F | DAM; optimum |
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66
(Unverified Data**) Zytel® FE270038 is a 40% glass fiber/mineral reinforced, heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.Information provided by DuPont Performan.. |
|||
Mold Temperature | 100 °C | 212 °F | DAM; optimum |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) Zytel® 73G35HSL BK262 is a 35% glass fiber reinforced, heat stabilized, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 100 - 130 °C | 212 - 266 °F | |
Lanxess Pocan® T 7141 000000 PET + PBT, 40% Glass Fiber/Mineral PET + PBT, 40% glass fibers/mineral, injection molding, improved flowability, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
Mold Temperature | 100 - 120 °C | 212 - 248 °F | |
LATI Latiohm 87/28-05 PD01 G/10 PC, 10% Glass Fiber Reinforced Semiconductive/dissipative product based on Polycarbonate (PC). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Mold Temperature | 100 °C | 212 °F | |
Taiwan PU Corporation PPG CPU-2079 Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Mold Temperature | 100 °C | 212 °F | |
Taiwan PU Corporation PPG CPU-2095 Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Mold Temperature | 100 - 110 °C | 212 - 230 °F | actual surface temp |
Unitika TERRAMAC TE-8210 Polylactic Acid (PLA) High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Mold Temperature | 100 °C | 212 °F | Injection Molding; ISO 10724 |
Covestro Apec® 1745 Polycarbonate Easy to demoldsuitable for superheated steam sterilization up to 143 °C as well as for pharmaceutical applications according to United States Pharmacopeia (USP) XXII Class VIsoftening temperature (.. |
|||
Mold Temperature | 100 °C | 212 °F | Injection Molding; ISO 10724 |
Covestro Apec® 2095 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=203 °CPreprocessingMax. Water content |
|||
Mold Temperature | 100 °C | 212 °F | Injection Molding; ISO 10724 |
Covestro Apec® 2097 Polycarbonate Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=202 °CPreprocessingMax. Water content |
|||
Mold Temperature | 100 °C | 212 °F | DAM; optimum |
DuPont Performance Polymers Zytel® PLUS PLS95G35DH1 BK031 Nylon Zytel® PLS95G35DH1 BK031is a high flow 35% glass reinforced PA using SHIELD Technology, only from DuPont, combining excellent surface appearance, excellent welding and fatigue retention, exceptiona.. |
|||
Mold Temperature | 100 °C | 212 °F | DAM; optimum |
DuPont Performance Polymers Minlon® EFE6096 GY090A Nylon 66
(Unverified Data**) Minlon® EFE6096 GY090A is a 15% mineral reinforced impact modified nylon 66 resin.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 100 °C | 212 °F | Optimal |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Conditioned) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
Mold Temperature | 100 °C | 212 °F | Optimal |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Mold Temperature | 100 °C | 212 °F | Optimal |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Mold Temperature | 100 °C | 212 °F | Optimal |
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Conditioned) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Mold Temperature | 100 - 130 °C | 212 - 266 °F | |
Akro-Plastic Akromid® T1 GF 40 9 (3499) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Mold Temperature | 100 °C | 212 °F | Optimal |
BASF Ultraform® N2720 M63 30% Mineral Filled POM Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF |
|||
Mold Temperature | 100 - 150 °C | 212 - 302 °F | |
LATI LAESTRA G/40-V0CT1 40% Glass Fiber Reinforced, Elastomer Modified, Flame Retardant Syndiotactic Polystyrene (SPS) Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |
|||
Mold Temperature | 100 °C | 212 °F | DAM; optimum |
DuPont Performance Polymers Zytel® 73G30TGI BK267 Nylon 6
(Unverified Data**) Zytel® 73G30TGI BK267 is a 30% glass fiber reinforced, toughened, black polyamide 6 optimized for gas injection molding process.Information provided by DuPont Performance Polymers |