Processing Properties Metric English Comments
Nozzle Temperature 232 - 243 °C
450 - 469 °F
Nylene® 401, Nylon 6
Injection molding grade. Dry As Molded. Nylene 401 is recommended for general purpose nylon molding applications in both thin and heavy sections. Nylene 401 has high flow characteristics at minima..
Nozzle Temperature 232 - 243 °C
450 - 469 °F
Nylene® 401, Nylon 6, at 50% Relative Humidity
Injection molding grade. Nylene 401 is recommended for general purpose nylon molding applications in both thin and heavy sections. Nylene 401 has high flow characteristics at minimal processing temp..
Nozzle Temperature 232 - 243 °C
450 - 469 °F
Nylene® 401D, Nylon 6
Injection molding grade. Dry as molded. Nylene 401D is a specially formulated nylon 6 molding resin possessing outstanding flow characteristics. Nylene 401D is ideally suited for applications requi..
Nozzle Temperature 232 - 243 °C
450 - 469 °F
Nylene® 402 Nylon 6
Injection molding grade. Dry as molded. Nylene 402 is a high monomer resin which offers outstanding toughness and flexibility. Nylene 402 exhibits excellent flow properties at temperature and press..
Nozzle Temperature 232 - 243 °C
450 - 469 °F
Nylene® 404 Nylon 6
Injection molding grade. Dry as molded. Nylene 404 is a heat stabilized version of 401 which is recommended for general purpose nylon molding applications in both thin and heavy sections. In additi..
Nozzle Temperature 232 - 243 °C
450 - 469 °F
Nylene® 404 Nylon 6, 50% RH
Injection molding grade. Nylene 404 is a heat stabilized version of 401 which is recommended for general purpose nylon molding applications in both thin and heavy sections. In addition to protection..
Nozzle Temperature 232 - 243 °C
450 - 469 °F
Nylene® 406 Nylon 6
Injection molding grade. Dry as molded. Nylene 406 is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded f..
Nozzle Temperature 232 - 243 °C
450 - 469 °F
Nylene® 406 Nylon 6, 50% RH
Injection molding grade. Nylene 406 is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded from 406 have bet..
Nozzle Temperature 232 - 243 °C
450 - 469 °F
Nylene® 406F Nylon 6
Dry as molded. Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling..
Nozzle Temperature 232 - 243 °C
450 - 469 °F
Nylene® 406F Nylon 6, 50% RH
Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling molding resin. ..
Nozzle Temperature 232 - 243 °C
450 - 469 °F
Nylene® 409 Nylon 6
Dry as molded. Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles..
Nozzle Temperature 232 - 243 °C
450 - 469 °F
Nylene® 409 Nylon 6, 50% RH
Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid m..
Nozzle Temperature 232 - 243 °C
450 - 469 °F
Nylene® 452 Nylon 6
Dry as molded. Injection molding grade. Nylene 452 is a plasticized, injection molding nylon for use in applications requiring high flexibility, and excellent toughness and abrasion resistance. Bec..
Nozzle Temperature 232 - 243 °C
450 - 470 °F
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 232 - 243 °C
450 - 470 °F
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 232 - 243 °C
450 - 470 °F
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 232 °C
450 °F
Injection
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Nozzle Temperature 232 °C
450 °F
Lubrizol ESTALOC® 59300 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro..
Nozzle Temperature 232 °C
450 °F
Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy
Type: Estaloc® 61225 Alloy RETPU is a polyester-type thermoplastic alloy.Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.Uses: Injection molding.Availa..
Nozzle Temperature 232 - 274 °C
450 - 525 °F
LTL Color Compounds ColorFast® FRPA100X Polycarbonate-ABS Alloy
V-0 rated polycarbonate-ABS alloy, excellent toughness and light stabilityAll information provided by LTL Color Compounders, Inc.
Nozzle Temperature 232 - 274 °C
450 - 525 °F
LTL Color Compounds ColorFast® JCT1000 Polycarbonate-ABS-SMA Alloy
Unique PC/ABS/SMA alloy with improved processing and reduced plate-outAll information provided by LTL Color Compounders, Inc.